Electronics Forum | Mon Oct 22 11:47:59 EDT 2007 | brulal1
Thank you guys for your help, I do not clean any on my assemblies who are build by the SMT an wave soldering department, we do used liquid fluxes Kester 951 and cored wire keester 245, usually it�s for batteries connector, led, terminal and wire rap
Electronics Forum | Mon Oct 22 15:41:39 EDT 2007 | davef
Bruno The real question about your troop using Kester 951 wave solder flux on boards is: how is the flux applied and controlled. See, when you apply this flux with your wave solder fluxer, it is ideally applied in a metered fashion with your fluxer
Electronics Forum | Tue Sep 21 02:51:06 EDT 1999 | Mohammed saad
Thank you all for your help. about your question Wolfgang, I am using no-clean solder paste from Kester. Mohammed | | Hi all, | | | | We have a little discussion here about the suitable flux for a certain process, as all of us are beginners we ne
Electronics Forum | Wed Aug 30 23:45:28 EDT 2000 | Ramon I Garcia C
Hi friends; Steve I'm using flux Kester 959, my top temperature is 187 celcius degrees, my e-mail is ramigary@smtnet.com, Travis I'll check the pcb for contamination, but how may I clean the pcb? may I use alcohol? Nance I cleaned the pipes of the