Electronics Forum | Sat Jul 29 02:05:39 EDT 2017 | benny
We now offer free expedite for PCB prototype. Min $5 for Standard 1-2 layers board with 24-48H lead time http://www.allpcb.com/T2 Min $34.78 for Standard 4 layers board with 48-72H lead time http://www.allpcb.com/T2 We thi
Electronics Forum | Mon Oct 29 05:14:18 EDT 2018 | vipcircuit
This is Joe from Shenzhen Vip Circuit Co,. Ltd.-- a leading PCB and PCBA manufacturer in China. Why choose Vipcircuit ? 1. PCB fabrication with 100% ET and AOI testing,certified by ISO, UL; 2. Special material like Rogers,Arlon,Taconic,Aluminum base;
Electronics Forum | Tue Feb 03 14:19:29 EST 2009 | grics
I would agree if you have a board to setup the process. But sometimes this doesn't work... If for some reason if the customers AVL has a Lead Free BGA and I am running Leaded paste (yes this really happens!), you will need to run hotter to get your
Electronics Forum | Wed Jul 05 05:07:51 EDT 2017 | heros_electronics
Hi Claire, Is it a 4G smart phone? Generally, 4G pcb board is HDI pcb with laser drilling and small line width and space, and not all PCB suppliers can manufacture because HDI PCB has special requirements for equiment, and small factory can not
Electronics Forum | Fri Dec 23 23:29:17 EST 2005 | azbvc
Slaine, thank you for sharing..
Electronics Forum | Fri Dec 23 06:09:04 EST 2005 | Slaine
good report showing lots of sections and compairng differnet pcb finishes http://www.smartgroup.org/experience/experience%20report%202005.pdf
Electronics Forum | Sat Dec 24 08:26:41 EST 2005 | GS
Thank you, very intersting. Seen they've experimented also Sn Cu Ni on wave solder. Rgards............GS
Electronics Forum | Mon Dec 30 08:14:45 EST 2013 | jax
I was unaware of any Pb-Free process capable FR-1 laminate... not to mention capable of Though Hole plating that would be expected when wave soldering. What is the Td and Z-expansion for the laminate you are using?
Electronics Forum | Mon Aug 30 16:10:10 EDT 1999 | Dave F
| I have looked through the IPC web page and surfed to frustration. Can somebody give me a lead? | Brian: We don't use an etched board. We use a special stencil, described below and print on bare copper laminate. 3 Solder Wetting Test. Recogniz
Electronics Forum | Mon Dec 30 02:05:08 EST 2013 | mysmt
Hello, I am facing intermittent delamiantion effect in FR1 type laminate after wavesoldring.Bath temp. is 255 degees cel.Preheater temp is also controlled (110 deg cel. on top side before passing on solder bath). Thanks,
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830