Electronics Forum | Fri Mar 26 13:02:18 EST 1999 | Scott McKee
Sorry, in the following message I'm agreeing with Graham - not Greg... | | I am looking into replacing another business division's Acrylic coating process with our Urethane coating process. Unfortunately, MIL-I-46068 doesn't differentiate AR/UR's p
Electronics Forum | Thu Mar 25 19:19:08 EST 1999 | Graham Naisbitt
| I am looking into replacing another business division's Acrylic coating process with our Urethane coating process. Unfortunately, MIL-I-46068 doesn't differentiate AR/UR's performance, and the MFR data sheets don't match up at all (they each spec
Electronics Forum | Mon Mar 29 04:36:49 EST 1999 | Graham Naisbitt
Just for the record folks, The customer I believe may be manufacturing stuff for refuelling rigs of various forms. This being the case, the coating would need to be resistant against fuels and oils. The UR material (at least ours!) is able to resi
Electronics Forum | Mon Mar 29 19:17:47 EST 1999 | Scott McKee
How true, AR would not be the right choice... Scott | Just for the record folks, | | The customer I believe may be manufacturing stuff for refuelling rigs of various forms. | | This being the case, the coating would need to be resistant against f
Electronics Forum | Fri Mar 26 12:59:51 EST 1999 | Scott McKee
| | I am looking into replacing another business division's Acrylic coating process with our Urethane coating process. Unfortunately, MIL-I-46068 doesn't differentiate AR/UR's performance, and the MFR data sheets don't match up at all (they each spe
Electronics Forum | Tue Jul 19 09:18:14 EDT 2011 | davef
Could this be an opportunity to explore the use of cartridge-type paste dispensers? Or maybe a reason to keep working over the weekend. * Re-Storing & Re-Using “Used” Solder Paste. Though not a recommended practice, used solder paste from the stenci
Electronics Forum | Wed Mar 14 16:01:39 EST 2001 | Rob Fischer
Not necessarily. Maybe just a little over > sensitive...? > > I though Bill provided > considerable insight relative to the process and > the original question. There was a good answer in > there. I also thought that he provided more > specifi
Electronics Forum | Tue Mar 16 05:11:47 EST 1999 | Charles Stringer
| | AVX and a few other companies make these chip transient voltage suppressors (TVS) parts that are a real *PAIN* to use. According to AVX: | | "Due to the semiconducting nature of the doped Zinc Oxide (ZnO) ceramic material, SMT TransGuard
Electronics Forum | Wed Jul 22 12:47:23 EDT 1998 | Earl Moon
| I'm trying to put together a set of design guides for use for new designers | in house or to be sent out for contracted layout work. I would like to start with a top ten list of things that will go wrong if rules aren't available. For example testp
Electronics Forum | Thu Jul 13 22:20:38 EDT 2000 | Dave F
=10 mils larger than lead 3 silk screen legend text weight >=10 mils 4 pads >=15 mils larger than finished hole sizes 5 place through hole components on 50 mil grid 6 no silk screen legend text over vias (if vias not solder masked) or holes 7 so