Electronics Forum | Tue Feb 22 00:43:13 EST 2005 | valuems
try alcohol or a mixture of alcohol and water (50%x 50%)
Electronics Forum | Mon Jan 24 20:20:24 EST 2011 | eadthem
having a mixture of ISP and browser problems today. Delete Me
Electronics Forum | Tue Sep 19 14:39:55 EDT 2006 | ppcbs
I have some Engelhard E-74 Potassium Gold Cyanide and related chemicals I use to make a small high concentrate plating bath for swab plating. I lost my bath mixture instructions and find that Engelhard no longer supports this product. Does anyone h
Electronics Forum | Thu Dec 04 12:24:35 EST 2008 | jdumont
We have the same Asymtek machine, same Humiseal product, same bubbling issue on touch ups. Ive found that very light pressure and a thinner mixture usually yields good results for us. Generally I dip the brush in the mixture and let it drip near wher
Electronics Forum | Fri Feb 18 12:00:08 EST 2011 | dennisfo
That has also been the standard here. We have a urethane line which pulls a vacuum on the mixture before transfering to the can. I plan on testing this out before receipt of the 73 thinner. I've also received some feedback with indication that the mi
Electronics Forum | Wed Mar 14 07:30:14 EDT 2007 | davef
So, you toss whatever is on the stencil every 8 hours. Correct? How long has it been on the stencil? * If that particular paste has been on the stencil for 8 hours, we'd agree to toss it too. * If paste has been on the stencil for less than 8 hour
Electronics Forum | Wed Jan 21 10:13:14 EST 2004 | ADAM
What is the most effecient form of heating ,ie calrod, IR, convection , or a mixture ? to produce a good thermal profile on a wavesoldering system on thermally challenging multi-layered boards? Thanks Adam
Electronics Forum | Fri Jan 23 03:19:23 EST 2004 | Erv
We have very good results with a mixture. Lower 1st and 2nd preheat is convection, 3rd lower is calrod. No upper 1st and 2nd, 3rd upper is IR. With this combination I have found no challenge that could not be turned into a good profile.
Electronics Forum | Tue Sep 27 11:46:02 EDT 2005 | jimby
surface tension of solder mask material on the board. Need to rough it up prior to board assembly. Use Silica (cabosil) and IPA mixture and rub
Electronics Forum | Wed Aug 27 23:00:55 EDT 2008 | omid_juve
i mean that the parts that we have here is ROHS compliant(pb free)but the process that we have(the type of solder paste & the surface finish of the board has pb in its mixture) this is not the cause of problem ?