Electronics Forum: no clean cleanliness requirements (Page 1 of 9)

Cleanning no clean residu

Electronics Forum | Mon Oct 22 08:54:27 EDT 2007 | rgduval

Michael, You're right, of course. A major mis-type on my end. What I meant to say is that no-clean fluxes are designed to not _require_ cleaning to meet industry cleanliness standards. Cheers ..rob

Cleanning no clean residu

Electronics Forum | Fri Oct 19 13:57:17 EDT 2007 | Michael Konrad

Hi Rob, I must take issue with your statement �By definition, no clean solder can be not-cleaned�. All no-clean fluxes can be cleaned. Whether or not one cleans no-clean depends on a variety of factors. More than eighty percent of all post reflow

cleaning of no clean flux

Electronics Forum | Wed Aug 10 07:55:21 EDT 2005 | ajaydoshi

we are using heareous F381, F352 no clean solder paste. specially in qfp for high frequency board we observe that cleaing / removing of ' no clean flux 'is require. if we do not clean same most of time after all test & envioumental test it shows pin

cleaning of no clean flux

Electronics Forum | Wed Aug 10 08:10:39 EDT 2005 | davef

Comments are: * Sounds like it's necessary to clean "heareous F381, F352 no clean solder paste" in your application. Consider a paste that may be better suited to your application. * If you're cleaning "low residue flux", consider using an organic ac

Re: water soluable or no clean flux?

Electronics Forum | Tue Sep 21 02:51:06 EDT 1999 | Mohammed saad

Thank you all for your help. about your question Wolfgang, I am using no-clean solder paste from Kester. Mohammed | | Hi all, | | | | We have a little discussion here about the suitable flux for a certain process, as all of us are beginners we ne

Re: water soluable or no clean flux?

Electronics Forum | Mon Sep 20 09:02:34 EDT 1999 | Wolfgang Busko

| Hi all, | | We have a little discussion here about the suitable flux for a certain process, as all of us are beginners we need your advice. | | We are producing VGA cards and mother boards for PC's all components to be wave soldered are TH, the S

Cleaning after rework, no clean flux

Electronics Forum | Wed Feb 26 23:59:48 EST 2003 | Mike Konrad

Grant, No-Clean paste + IPA = White Residue! #1: Stop using IPA #2: Switch to either a solvent-based de-fluxing chemical or an aqueous-based de-fluxing chemical. If you are using an ultrasonic cleaner for your boards as stated, do not use sapon

Manufacturing and test room cleanliness

Electronics Forum | Mon Feb 05 10:12:32 EST 2007 | slthomas

The use of booties isn't required per se, just considered a standard step necessary to reach the 10,000 target. You also need to vacuum (central vac system, NOT exhausting into the room) daily, mop weekly, have a one piece floor, blah, blah, blah....

assembly cleanliness and ionic testing

Electronics Forum | Thu Feb 12 11:57:59 EST 2009 | jmiller

i have searched the forum for hours. read all the threads that deals with cleanliness and ionic testing. (http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=40295) (http://www.smtnet.com/forums/Index.cfm?CFApp=1&Message_ID=22603) (http://www.

High Frequency Product.... malfunction when using no clean paste

Electronics Forum | Wed Jun 16 08:56:34 EDT 1999 | Vic Lau

Do anyone have any experience on assembling high frequency product, 1.8GHz or 2.4GHz. In our production line, we manufacture 1.8GHz product with using no clean paste (RMA type) for reflow and no clean wire for rework. In our functinal test,either a