Electronics Forum | Mon Feb 27 19:48:32 EST 2006 | stepheniii
I'm not sure that would be valid. My understanding was that solids were trapped by other non-active flux residue. Which is why you can leave them on and why you see white residue after washing. I think the ROSE test would release particles that woul
Electronics Forum | Thu May 11 11:25:56 EDT 2017 | davef
Key to Rosin Fluxes [from SUPERIOR FLUX & MFG. CO.] Type R (Rosin): Non-activated rosin flux for soldering copper. Residues are non-corrosive and non-conductive. Type RMA (Rosin Mildly Activated): Mildly activated rosin flux that contains no chlori
Electronics Forum | Fri Dec 17 03:38:53 EST 1999 | cklau
Hello Guys; I "ll like to add some comment on Mr John message , see below.. "Be sure that the components to be used on the bottom can take the maximum heat of the wave and the delta T of entering the wave."-John The required preheat temp , that i
Electronics Forum | Tue Jun 26 19:51:31 EDT 2001 | davef
Rosin. A hard, natural resin, consisting of abietic acid [and pimaric acids in Europe] and their isomers, some fatty acids, and terepene hydrocarbons. Rosin is extracted from pine tree stumps. It�s an organic material distilled from oleoresin in p
Electronics Forum | Mon Aug 17 02:57:47 EDT 1998 | Bob Willis
| | Looking for Suppliers of surface mount wetting balance equipment. | Bucky: Section 6 of the ANSI/J-STD-002 specification lists wetting balance suppliers. Dave F I like and continue to use the Multicore system. I have had many ours using the sys