Electronics Forum | Thu Jul 05 06:36:14 EDT 2001 | nifhail
Thanx Dave, I agree with you on the planning part...yapp!! the same guy who've thrown an old datecode components to me..now they did it again on the PCB. Well Dave, could you explain a little bit more about the "hi-test flux" that you mentioned ab
Electronics Forum | Thu Jul 05 06:38:35 EDT 2001 | Danial
Thanx Dave, I agree with you on the planning part...yapp!! the same guy who've thrown an old datecode components to me..now they did it again on the PCB. Well Dave, could you explain a little bit more about the "hi-test flux" that you mentioned ab
Electronics Forum | Wed Jul 04 10:40:51 EDT 2001 | nifhail
I have thousands of old datecode PCBs which has an Entek and HASL finished. Entek PCBs are about 6 � 1.5 years old and HASL boards are at 1 - 2 years old. To make it worse, some of them came in the loose form, no vacuum seal� nothin�. As for the HA
Electronics Forum | Thu Jul 05 11:14:04 EDT 2001 | caldon
We can offer two ways. We have a process control tool for OSP boards to validate the finish......but the dates yer talking may be best to take Daves F suggestion. NOW as far as the HASL finish goes...We may have your answer. We can Chemically revers
Electronics Forum | Thu Jul 05 19:39:19 EDT 2001 | davef
I had forgotten that it was you that was on the Sipad adventure. [But then again, who can keep track of yer aliases? ;-)] You just go from one adventure to the next. Expanding On Dave�s Hi-Test Flux Method Theory � PASTE: Yes, contact your favorit
Electronics Forum | Wed Jul 04 12:35:19 EDT 2001 | davef
I thought I responded this this a while ago, guess NOT!!! Wow, Dano yagot Entek boards that are that old!!!! Coo. Sounds kwazy that you�d end-up with that volume of old boards, but it�s probably one of those deals where correcting the problem keep
Electronics Forum | Mon Sep 09 07:51:00 EDT 2002 | yngwie
I don't know when I can get done with an old datecode material..anyway, thanx for the help guys. cheers.. zambri
Electronics Forum | Tue Jun 26 12:39:08 EDT 2001 | danial
Our mother company shipped to us a lot of old datecode material and upon running them in the line we experienced non-wetting condition, esplly on the 0402 ( not tombstone ) We have run a dip-and-look test but I guess the method is very subjective as
Electronics Forum | Tue Aug 14 12:18:02 EDT 2001 | nifhail
I experienced assembled boards delaminated after washed. You know...those old datecode PCBs that I was talking about a few weeks back ? I was forced to use it, and of course prior using it I've baked them. I've baked them at 125 Deg for 4 hours and/
Electronics Forum | Fri Jun 29 05:50:27 EDT 2001 | nifhail
Thank Dave, your information was really helpful. Now that I have another few thousands of old datecode PCBs which has an Entek and HASL finished. Entek PCBs are about 6 � 1.5 years old and HASL boards are at 1 - 2 years old. To make it worse, s