Electronics Forum | Wed Mar 30 17:32:55 EDT 2011 | gaz
Hi, We are using ws488 sn100c paste. Anyone have a profile for a 5 zone oven that has worked well for you?
Electronics Forum | Tue Apr 05 12:18:25 EDT 2011 | gaz
That's very helpful, and much appreciated. I know it's a long shot, but I don't suppose you know what paste they are using with these settings. I am testing with sn100c ws488. Thanks! kinos
Electronics Forum | Tue Apr 05 15:32:49 EDT 2011 | grahamcooper22
It is one of our pastes...Almit LFM48 W TM-HP, a high reliability no clean solder paste based on SAC305 with a size 4 powder. It's a paste that works so well we have thousands of users of it worldwide. Why are you using SN100C alloy paste ? I imagin
Electronics Forum | Mon Aug 26 09:50:32 EDT 2002 | zanolli
I want to ascertain the oven profile required for through hole connectors with solder pre-forms. I need to get double sided PCB�s made for that purpose. What is the best way to get these PCB�s made to simulate real world conditions?. Should I leave a
Electronics Forum | Mon Aug 26 20:33:50 EDT 2002 | davef
Not as such. Generally, people tailor their profiles to produce glam solder connections on their boards. Search the fine SMTnet Archives for discussion on the factors affecting solder reflow recipes. What is the best way to get these PCB made to s
Electronics Forum | Wed Aug 28 18:08:07 EDT 2002 | MikeF
This looks like it may be a good application for an Air-Vac or Wenesco type solder station. It is a solder pot that has a small motor to pump solder up through a chimney. You can put different nozzles on the top of the chimney, so you only apply sold
Electronics Forum | Tue Feb 01 09:54:23 EST 2005 | jbrower
Hi Frank, we're still going to go with FR4 as our prefered material. Our board thickness is .062. We use an on shore and off shore vendor. Prototron I believe offers an immersion tin and excellence in china? offers an immersion tin finish. We fou
Electronics Forum | Mon Sep 10 14:42:42 EDT 2007 | cyber_wolf
How big is the cap ? We successfully reflow caps that measure aprrox .750" x 750" at the base and are .678" tall. The ovens we use are Vitronics XPM's.(1230,1040 and 930) We also process these caps through our Omniflow 10. As stated, oven length wi
Electronics Forum | Mon Sep 10 11:16:37 EDT 2007 | russ
Can you implement a longer soak? how many feet of heat do you have in oven? Russ
Electronics Forum | Thu Jun 19 12:07:09 EDT 2008 | ck_the_flip
You answered your own question! Vapour phase is the way to go for this. Conventional ovens won't allow this, unless you find away to defy Physics. That's an absurd constraint to begin with: 200C. Most Sn-Pb profiles require 205 - 210 minimum for