1. To protect the nickel and copper under gold plating from oxidization before soldering. Gold plating can extend the PCB self-life and improve the solderability for 2nd re-flow. 2. Provide a good bonding strength. For Chip on Board process that Gol
Electronics Forum | Thu Aug 21 22:10:07 EDT 2003 | adlsmt
Well, for some reason the board house will pay for the boards but has some issue with paying for the parts on them. Why am I not supprised? Perhaps I have mis-diagnosed the problem. We have found two different board p/n's with the same type of defec
Electronics Forum | Tue Dec 01 07:24:44 EST 1998 | Earl Moon
| Hi folks , | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspection
Electronics Forum | Tue Dec 01 07:54:49 EST 1998 | kallol chakraborty
| | Hi folks , | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspec
Electronics Forum | Tue Dec 01 09:02:18 EST 1998 | Earl Moon
| | | Hi folks , | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our in
Electronics Forum | Fri Dec 04 20:26:34 EST 1998 | kallol Chakraborty
| | | | Hi folks , | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Ou
Electronics Forum | Fri Dec 04 20:37:45 EST 1998 | kallol chakraborty
| | | | | Hi folks , | | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most
Electronics Forum | Mon Nov 30 23:45:20 EST 1998 | Kallol Chakraborty
Hi folks , Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspection /te
Electronics Forum | Tue Jul 18 22:11:13 EDT 2006 | davef
Aping Russ' reply: * ~70% of the time solder on gold fingers is caused by poor printing and handling processes. * ~25% of the time solder on gold fingers is caused by poor thermal recipe when soldering. * ~5% of the time solder on gold fingers is cau
Electronics Forum | Tue May 13 06:57:10 EDT 2003 | davef
Your vendor site is totally correct. 2Ag is an excellent solder, but it does nothing to prevent tin and gold from reacting chemically. An earlier poster is correct gold goes into solution in liquid solder very fast, less than a second. Gold and ti