PCb vacuum seal puncture

Electronics Forum | Thu Jul 18 12:05:19 EDT 2002 | yngwie

Experts, Today I received PCB in a punctured vacuum seal bag. the Humidity indicator change the colour to pink at 60%RH mark. The brd finish is Entek. Earlier our intention to get the board vacuum seal is because we want to ensure that the is no fr

PCB with ENIG plating shelf life?

Electronics Forum | Wed Nov 09 07:43:12 EST 2022 | micropak

ENIG boards have low shelf life as oxidation starts showing up quickly on the solderable areas. We usually keep them vacuum packed till they are ready to be assembled. Most PCB manufacturers will send them vacuum packed.

dry oven

Electronics Forum | Wed Aug 14 13:54:54 EDT 2002 | DenM

Larry, You can try one of two approaches, a bake above 100C will drive off moisture or use a vacuum bake. The vacuum bake process is slow since there is less/no air to conduct the heat. In the hybrid industry the standard vacuum bake was 16 hours at

Do yo have to bake unused bare boards or just Vacuum Pack?

Electronics Forum | Sun Aug 27 20:30:53 EDT 2006 | darby

AJ, We use all ENIG boards. After opening, any remaining boards are kept in low humidity keeping cabinet. I have never experienced a problem using this method I think the longest I have kept them this way is eighteen months. We also store any open tr

PCB with ENIG plating shelf life?

Electronics Forum | Wed Nov 09 17:18:08 EST 2022 | emeto

If they are vacuumed and they approach 6months or 1 year mark, what would you do?

Do yo have to bake unused bare boards or just Vacuum Pack?

Electronics Forum | Fri Aug 25 07:42:29 EDT 2006 | davef

Our sympathies about the ENIG boards. B:) So, you cut the end off the barrier bag, take 200 boards, heat seal the end of the bag and restock it, build the 200 boards and ship them, right?

Do yo have to bake unused bare boards or just Vacuum Pack?

Electronics Forum | Mon Aug 28 07:28:07 EDT 2006 | davef

Mr Jarvis One experience with black pad makes you promise never to use ENIG again. It's nice that you have a supplier that has avoided that problem.

immersion Gold life span

Electronics Forum | Mon Jan 08 03:16:12 EST 2007 | oswald5087

hi' i need advise on immersion gold PCb shelf life. 1) what is the issue shelf life or expire for Immersion gold PCB? 2) How long we can keep the PCB? (with vacuum seal and without vacuum seal) 2) iF PCB expire, can we bake the immersion PCB? what t

immersion Gold life span

Electronics Forum | Mon Jan 08 17:32:47 EST 2007 | Board House

Hi Oswald, Shelf life with ENIG if vacuum sealed and kept in controled enviroment would be 12 to 14 months. Shelf life in shrink wrap - No recomended packaging, 6 moths. If Shelf life goes over the 12 -14 months - Baking ? I would not suggest re-b

HIC turn Pink for PCB-URGENT

Electronics Forum | Tue Jul 06 08:04:01 EDT 2004 | ANDREW

Thanks Dave, The surface finish is ENIG.Is it ok not to bake even though the HIC has changed color? What is the shelf life for ENIG boards?

  1 2 3 4 5 Next

pcb baking enig vacuum searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830