Electronics Forum | Thu Jul 12 02:15:53 EDT 2012 | thmeier

Check also the specs / recommendations of your PCB manufacturer. We bake boards 4h/120°C before reflow and after automated cleaning (it´s not FR4!) and also if we have to rework with the autometd rework- stations (massive IR underheating ,..). Regar

baking out pcbs after reflow process

Electronics Forum | Wed Jul 11 22:48:54 EDT 2012 | joeion

It is correct to remove moisture in PCB by baking. But I think the time and temperature is too little. According to our experience, it should be more than 60min at 120 centigrade degrees.

baking out pcbs after reflow process

Electronics Forum | Thu Jul 05 11:26:08 EDT 2012 | cobham1

I need help with how long do I need to bake out double sided PCB's that have been cleaned. The units will not be reworked but instead will be moved on to hand stuffing. I have looked in IPC CH-65B and J-STD-033C. I get information for parts if I am r

Re: silver finishes on pcbs

Electronics Forum | Wed Dec 13 10:24:52 EST 2000 | Wolfgang Busko

Hi Jack, I once tried this finish ( without changing any process parameters ) and encountered wetting problems even in the first reflow process. It was thought as cheaper alternative to Ni/Au we use for planarity reasons. Heard of the same problems

Re: silver finishes on pcbs

Electronics Forum | Thu Dec 14 10:14:04 EST 2000 | PeteB

Jacqueline, Asuming you mean immersion silver: Advantages - Very flat finish compared to HASL, more easily solderable than bare copper with OSP and more process tolerant than this in our experience, reasonable shelf life, cheaper than immersion gol

PCB & MSD Component baking oven

Electronics Forum | Fri Dec 03 04:11:47 EST 2010 | grahamcooper22

A baking oven over 100 C will be at zero humidity. Do you really need to store pcbs/devices at 200 C...this will surely harm some products ? IPC 33B01 allows storage of MSDs in a dry cabinet at less then 5%.....these can operate at room temp or 40 /

Re: silver finishes on pcbs - what about the wave?

Electronics Forum | Fri Dec 15 08:00:57 EST 2000 | Pete B

John, We regularly wave solder electroless silver finished boards (Alpha Level)with mixed SMD and through hole parts and do not have any problems. We have changed a number on PCB's from HASL to electroless silver, mainly for the benefits at SMD whe

Re: Is baking PCB necessary before solder process?

Electronics Forum | Thu Jul 29 12:33:38 EDT 1999 | Wolfgang Busko

| Currently, we are baking any PCB before process on SMT, the 'reason' is to dry any possible humidity that could be inner the PCB, it does not matter if the PCB is multilayer or not. We bake PCB's at 107C for 4 hrs and the board must be process into

PCB Baking after Wash

Electronics Forum | Tue Dec 09 10:04:36 EST 2008 | lazzara55

SMT-ypw: Does PWB supplier start to implement PWB drying packaging? B3: YES! The fabrication of the PCB involves a series of wet processing that requires counter-measures to remove moisure. While some of the PCB processes also include bake cycles th

Wash and bake of blank PCB's before assembly

Electronics Forum | Thu Jun 04 14:30:13 EDT 1998 | Igmar

I would appreciate any information concerning the wash and bake of blank Printed Circuit Boards before assembly. + Is it necessary to wash and bake PCB�s before assembly? + If any, what is the reason for wash and bake of PCB�s? + If any, what type of

  1 2 3 4 5 6 7 8 9 10 Next

pcb baking wet pcbs searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830