About the PCB gold finger contamination.

Electronics Forum | Wed Sep 18 22:53:24 EDT 2002 | davef

Please give us background on your situation, so that we can focus on the specifics, for instance: * This is a bare board problem, correct? Then, this contamination causes what the problems in your process? * What is the type [ie, FR4, CEM1, etc] of

solder on gold finger

Electronics Forum | Fri Apr 13 22:38:19 EDT 2001 | edylc

Hi , Could you be seeing the nickel under the gold plating because you are removing some of the Gold with the Kapton Tape....?? You mean , the adhesive properties of the kapton tape will cause the gold plating on the gold finger to be somehow peel of

solder on gold finger

Electronics Forum | Fri Apr 13 12:37:35 EDT 2001 | edylc

>>> gold finger was covered by a Kapton tape and it was done offline away from the Screen printer or rather from the SMT lines itself, we are using an ENIG Pcb's , the process doesnt need a wave soldering ....however at the final end of the line ,

Re: Solder on gold finger

Electronics Forum | Sun Jul 26 22:35:55 EDT 1998 | D.Lange

Masdi, Try board shunts. They are hi-temp rubber strips with grooves cut. They can be popped on and off with ease and are much faster than taping and considerably cheaper. They also work great for masking goldfingers prior to wave soldering. Contac

Gold finger touch-up paint

Electronics Forum | Tue Oct 26 12:18:53 EDT 1999 | Gary Kemp

We are having a discolorization problem with the gold fingers on our PCB's. I have been made aware that there is a gold touch-up paint (masking) that is available. Would anyone know where I can get my hands on some of it? Any help would be appreci

Re: no-clean mask for gold fingers

Electronics Forum | Sun Jan 31 23:03:57 EST 1999 | Dennis O.

| | hi, | | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier pr

About the PCB gold finger contamination.

Electronics Forum | Thu Sep 19 02:45:33 EDT 2002 | bugsjoe

Thank you ur reply Dave. Let me explain our COB workflow: 1. unpack PCB (FR4,LPI,HASL)(the thickness of gold and nickel we can't be find)(No SMT before) 2. clean the pcb by rubber 3. blow the pcb by di-ionic gun 4. attach die by adhesive gel 5. cure

About the PCB gold finger contamination.

Electronics Forum | Wed Sep 18 22:10:48 EDT 2002 | Joe Wong

I'm working China ,in my working factory is a electronic OEM factory and got COB and SMT. But recently, COB got a big problem because the PCB gold finger got a contamination, that make us got a most defect product. So anyone can answer me how to clea

Gold plating thickness on gold finger

Electronics Forum | Thu Oct 07 20:34:48 EDT 1999 | Tony Huang

Hi, Does anybody know what is the minimum gold plating thickness on the PCB goldfinger required by the industrial specifications - IPC, Bellcore, etc. Where can I find the information? Appreciate for the help! Thanks, Tony

About the PCB gold finger contamination.

Electronics Forum | Thu Sep 19 20:28:59 EDT 2002 | bugsjoe

* What kind of the eraser can clean clearly?I've been use the eraser but the defect still present.

  1 2 3 4 5 6 7 8 9 10 Next

pcb gold finger mask searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830