Electronics Forum | Sat Apr 21 04:39:45 EDT 2012 | brotakul
I am using different equipements for SPI such as Koh Young and Cyber Optics machines. I am looking for implementing a general procedure (SWP) for setting LSL's and USL's on the products on which the customer does not specify any limits on the solder
Electronics Forum | Mon Jan 30 05:58:39 EST 2017 | rob
Hi all, > > Am new to SMT here. > > I have a very > thin laminate substrate which around 120um > thickess. Being that thin, warpage is constantly > an issue for us. > > For the solder printing part, > we have a number of problems. > > Being s
Electronics Forum | Wed Jul 09 16:01:10 EDT 2003 | russ
Mike, the one pad that is "small" definitely appears to be over etching (It looks like it was supposed to be much larger). What is the dims of this little bugger as compared to the Gerber? i would also tend to believe that there probably is some mask
Electronics Forum | Wed Apr 23 19:00:39 EDT 2008 | stevek
It depends on the laminate but a PWB is like any other MSL component. Some fab shops are only waranting standard FR4 laminates for 45-60 days when processed at lead free temperatures. The best thing I can say is to try some weight gain/loss experim
Electronics Forum | Sat Jul 28 08:37:52 EDT 2007 | davef
There is no good choice. Board Finishes: Industrial/Battelle Class 3 Environment [Reliability Knowledge Gaps: For use of Pb-free solders in High Reliability Applications, J Smetana, iNEMI Availability of SnPb-Compatible BGAs Workshop, March 1, 2007,
Electronics Forum | Wed Apr 01 04:34:41 EST 1998 | Alan Pestell
We are looking at reflow soldering some Flexi-rigid pcbs. I have heard that IR reflow soldering can make the Polyimide "self heat" and cause de-lamination. Does anyone have any info.
Electronics Forum | Sun Apr 05 09:46:47 EDT 1998 | Earl Moon
| We are looking at reflow soldering some Flexi-rigid | pcbs. I have heard that IR reflow soldering can make the Polyimide "self heat" and cause de-lamination. | Does anyone have any info. The thermal problems associated with polyimide rigid/flex de
Electronics Forum | Fri Feb 01 11:58:28 EST 2002 | Romain
the PCB vendor is Multek in germany he made some measures about P content in Ni layer. What is the normal level of Phosporous and what is the upper limit ? thanks Romain
Electronics Forum | Thu Jul 15 15:55:41 EDT 1999 | nards penalosa
| | We have been encountering diminishing ball shear readings these past few weeks, despite the fact that we did not change any ball shear tester parameter. Our reflow parameters are also within spec limits. ( 210-220 deg C max temp. and 40-60 sec d
Electronics Forum | Thu Jul 15 12:26:56 EDT 1999 | Earl Moon
| We have been encountering diminishing ball shear readings these past few weeks, despite the fact that we did not change any ball shear tester parameter. Our reflow parameters are also within spec limits. ( 210-220 deg C max temp. and 40-60 sec dwe
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830