Electronics Forum | Tue Sep 15 12:11:36 EDT 1998 | Bill Schreiber
Jeff, The use of flux thinner would only add another chemical to the process. Environmentally, that would not be a good idea. My guess is that you would only end up with "thinner jelly" anyway. Alcohol works well on RMA flux. When assemblers switch f
Electronics Forum | Thu Apr 19 15:22:34 EDT 2001 | jdtpfacreate
Spanky, It sounds like you are looking for a recipe to use when you do get an assembly in that has 0201's on it. We have worked with our customers worldwide in the development of the process to use 0201's. Most equipment manufacturers out there
Electronics Forum | Thu Aug 07 16:12:03 EDT 2003 | davef
We have been soldering lead-free components on the products with SnPb solder for 10 plus years. Over those years, TI has shipped 20 billion parts with Pd solderability protection. Turn-up the dial on your oven and push on to other things.
Electronics Forum | Wed Nov 11 13:51:19 EST 2015 | duchoang
Could you give us more details. Picture, profile, solder paste ...?
Electronics Forum | Mon Nov 09 06:28:03 EST 2015 | recard
Hi guys, we have a problem and I hope something can give nme some new information. We have big solderability problems with a gold plated board. We changed the paste already, but there is no improvement. Could the Vapor phase Technology cause the p
Electronics Forum | Tue Mar 31 05:26:14 EDT 2009 | d0min0
Hello, we had similar problem in the past - when we had to change PCB supplier from a batch of hundreds of boards (NiAu plated, SnPb process) we got 2-3 boards with paste wicking to components leads what we did, was to check the thickness of gold on
Electronics Forum | Fri Nov 11 22:14:11 EST 2022 | kumarb
I would certainly test the boards but from our experience, the vacuum sealed in room temp, no issues at all with our PCBs sourced from Suntak / PCB Founder / Fastprint / Yaxinda / JLCPCB well past the 12 month mark. We building boards purchased 5-10
Electronics Forum | Thu Mar 31 20:16:31 EDT 2011 | tkirk
We recently decided to try using a different source for our bare boards to save money. On two different batches of PCBs now from the new source, we are seeing beading including some serious enough to short out underneath 0805 parts. We have never re
Electronics Forum | Tue Feb 03 16:42:50 EST 2009 | cuperpeter
Hello All, > > I have a problem with nonwetting Au > finish after second cycle of reflow soldering > doublesided boards. Solder nonwetted pcb pads (is > wicked to component terminations) Either these > pads or some of non component pads became
Electronics Forum | Sat Jul 25 18:35:33 EDT 2015 | orbitcoms
I am looking for information regarding setting up an SMT assembly line. I have recently purchased a stencil paste printer, pick and place, and reflow oven. The main information I need is the paste selection and best finish material on the PCBs. I wil
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830