Electronics Forum | Thu Feb 10 11:29:19 EST 2011 | patrickbruneel
If you search the documents for tin whiskers it’s getting very interesting. Also you can find in the report that lead-free (SAC) solder is used. http://www.nhtsa.gov/staticfiles/nvs/pdf/NASA-UA_report.pdf This report also confirms that the board
Electronics Forum | Fri Dec 23 23:29:17 EST 2005 | azbvc
Slaine, thank you for sharing..
Electronics Forum | Sat Dec 24 08:26:41 EST 2005 | GS
Thank you, very intersting. Seen they've experimented also Sn Cu Ni on wave solder. Rgards............GS
Electronics Forum | Fri Dec 23 06:09:04 EST 2005 | Slaine
good report showing lots of sections and compairng differnet pcb finishes http://www.smartgroup.org/experience/experience%20report%202005.pdf
Electronics Forum | Tue Nov 18 07:22:56 EST 2008 | wewilldoit
Hi folks! TI told us that we are the only one with the following problem... We discovered a really bad wetting characteristic of some SMD ICs from BurrBrown. At the moment: XTR106 / INA118 / ADS7844. After the reflow process we found out that this pa
Electronics Forum | Mon Apr 15 12:22:21 EDT 2019 | cyber_wolf
You demonstrate it and record it by the report. The report contains the check off items that you defined in the protocol along with supporting data from the testing you did. This usually involves part numbers,data points, and photos. The report shou
Electronics Forum | Tue Apr 09 17:33:45 EDT 2019 | tey422
I just assigned to make an IQ/PQ/OQ validation report to prepare for a couple of new yet very simple medical assemblies we are to build for. I have no idea how to make this report. All I know is I have to come with the validation report for all the
Electronics Forum | Fri Nov 11 04:06:46 EST 2005 | arnold
we are manufacturer of molded type transformer. we have a trim and form process and its damage the pins of our units. the TIN insulation was being damage so we decide to immediately solder (wave soldering) the units to avoid oxidation. my question is
Electronics Forum | Sun Mar 03 22:15:13 EST 2002 | caldon
RPS (Robtic Process Systems - I think) Makes a system called a Wet Balance tester. This machine is useful for Solderability on PCB sections and Components. Also for more info please go to http://www.empf.org/html/empfset.htm and down load Decemeber
Electronics Forum | Wed Nov 06 08:59:51 EST 2002 | rmorford
This defect is there after reflow. My first thought was that the boards had some sort of contamination, too. This is a new PCB manufacturer for this board (they have been making other boards for us). But... why only on the connectors -- why only o
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830