Electronics Forum | Fri Jan 31 12:42:07 EST 2003 | russ
Has anyone ever depaneled a PCB that is .135" thick using mousebytes? If so, what would be the right drill pattern to use? Thanks in advance Russ
Electronics Forum | Sat Feb 01 16:11:24 EST 2003 | Paul Smith
I would suggest scoring if the profile allows, leaving residual material of circa 40 - 50 mil - That is what I do on a 125mil thick PCB width of the pis is approx 200 mil Mouse bites on a board as thick as 135 mil will mean its extremly difficult to
Electronics Forum | Tue Apr 23 13:43:29 EDT 2013 | dyoungquist
PCB breakaway tabs, such as the borders around panels, often do not have any metal on them. These would have no recycle value. Our local metals recycling company has now started to recycle PCBs, loaded or unloaded. They only pay $0.08 (USD) per po
Electronics Forum | Tue Apr 23 10:43:53 EDT 2013 | ccross
Can anyone point me to a company that can recycle the breakaway material from our PCBs? Thanks
Electronics Forum | Thu Jan 03 14:05:11 EST 2008 | fsw
Patrick, thnx for your info. The tabs will be soldered on a PCB pad just like an SMT component. Will let all know once I have some more info.
Electronics Forum | Thu Jan 03 17:39:34 EST 2008 | flipit
Why are you using stainless steel? Corrosion resistance? Can the stainless be gold plated? I think this can occur metallurgically. Maybe nickel first then gold. Why are you removing the nickel? Nickel is somewhat magnetic. Had an application onc
Electronics Forum | Thu Jul 27 10:57:35 EDT 2017 | fkn
We make pcb depaneling equipment and many of our customers do a combination of tab routed panels with pre-score in order to speed up the singulation process. If you like, I can send you a picture of an example. Regards Klaus Heimann FKN Systek Tel.
Electronics Forum | Thu Aug 31 09:04:23 EDT 2017 | hxamalia
Hello ALL, Good day , it is Amalia from HX Circuit Technology Co.,Ltd in China, we are a prefessional PCB factory with many years. We are focusing on quick lead time for PCB with good service . please contact with me now ,thanks Email: amalia@hx-c
Electronics Forum | Thu Aug 22 07:48:30 EDT 2002 | Dave Milk
While separating individual pcbs from a panel, operators have caused delamination of the edge of the board, at the tabs that were cut. How can these boards be repaired? The delamination causes them to fail J-STD-001C 9.2.1.1.d. Also, what would yo
Electronics Forum | Mon May 17 10:04:35 EDT 2010 | jamyboy
We are caught in a dilemma of PCB tab recycling....does anyone out there recycle their removed PCB tabs, or do you trash them?
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830