Electronics Forum | Fri Jul 26 12:41:25 EDT 2013 | gallionc
We've had similar "disputes" with our quality department. A technical engineer from Nordson told me that the flourescents in the coating can look faint depending on the angle in which you look at the surface as well as how solder joints reflect the
Electronics Forum | Thu Aug 07 12:58:59 EDT 2014 | kahrpr
One of the things you need to know are the parts you are building Flight Critical. Meaning if the board fails will it bring down the aircraft. Or non critical meaning one of the over head light will fail as an example this determines how much latitud
Electronics Forum | Thu Oct 21 23:20:05 EDT 2010 | camtechpcb
According to the Trichromatism.Half red and half blue will get purple.But the trichromatism only apply to color light. The red and blue soder mask are coloring material.Both of them absorb light.You mixed them up,so you lose blue and red,and get grap
Electronics Forum | Thu Nov 22 09:14:06 EST 2007 | paulallan
Does anyone have any experience in point to point laser soldering and laser light reflecting off of SMT component 'J' leads down on to the laminate. This appears to be a random situation we cannot understand nor control.
Electronics Forum | Mon May 16 17:23:28 EDT 2005 | alandra516
Fred, call me I may be able to shed some light on what to look for. Glenn 903-892-5636
Electronics Forum | Fri Oct 30 12:48:59 EDT 2009 | dannou
I've been the AOI programmer for around 5 years now. The equipment I use is the Orbotech VT-9300 & VT-9500 systems. The programming isn't too difficult, mostly Grey-scale shadow measurement through application algorithms. Three levels of lighting an
Electronics Forum | Fri Apr 22 11:21:42 EDT 2005 | HUH
There are several types of lasers to do laser soldering. Panasonic also has a high intensity light that can solder as well. I've tried em' all and two over whelming things stand out when it comes to this type of soldering. #1 is preheat. It seems
Electronics Forum | Tue Jun 13 12:03:10 EDT 2000 | Chris May
Jason, If 225C is the topside temp of your board just prior to hitting the wave, I would say this is too high. Your flux suppliers data sheet should tell you an ideal topside temp for good flux activation, probably around 190C. According to the Bi
Electronics Forum | Thu Apr 17 13:00:28 EDT 2003 | Takfire
Russ, The caps are 0603 case size. I am not sure about the manufacturing details, as I work for the capacitor supplier. The manufacturing details are unclear at the moment, as the customer (South of the border) has not released such detailed inform
Electronics Forum | Thu Jul 03 12:03:00 EDT 2003 | slthomas
So, there is a crack or gap between: * Solder and component termination. Bingo Correct? Describe: * Coarseness / smoothness of the metal on the termination underneither the crack. * Solder left on the termination. Unfortunately at 45X I can't rea