Electronics Forum | Tue Jan 26 19:43:02 EST 1999 | Ross Berntson
| hi, | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier proces
Electronics Forum | Tue Jan 26 19:43:26 EST 1999 | Ross Berntson
| hi, | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier proces
Electronics Forum | Sat Jan 23 12:37:35 EST 1999 | parag palshikar
hi, i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier process ut
Electronics Forum | Mon May 18 17:59:06 EDT 1998 | Richard Jackson
I've tried every thing I can think of. Do you have any Ideas? What I have is micro balls on the gold fingers of panelize boards. These balls only appear on the gold finger. Or at least I can only find them on the gold fingers. What I have tried so
Electronics Forum | Wed Jan 27 11:42:50 EST 1999 | John Zisa
| hi, | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier proces
Electronics Forum | Sat Jan 23 16:07:20 EST 1999 | Steve Gregory
| hi, | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier proces
Electronics Forum | Wed Jan 27 20:34:13 EST 1999 | parag palshikar
| | hi, | | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier pr
Electronics Forum | Mon Jan 25 21:43:04 EST 1999 | Dave F
| hi, | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier proces
Electronics Forum | Sun Jan 31 23:03:57 EST 1999 | Dennis O.
| | hi, | | i am working towards developing a no-clean process for a customer at contract manufacturing facility. the assemblies have gold fingers on them. these are masked to prevent from any damage to them during reflow soldering. the earlier pr
Electronics Forum | Tue May 19 12:54:55 EDT 1998 | Richard Jackson
| We had a similar problem. But whenever the solder came from the screen printer the solder would wet to the gold fingers, with the help of residual flux. But the problem is balls, that I assume are not wetted to the gold fingers but instead are jus