Electronics Forum: poor hasl (Page 7 of 9)

Re: HASL - again?

Electronics Forum | Fri Jun 18 17:19:48 EDT 1999 | Jason Gregory

| | | | | Now don't everyone jump on this at once, but it seems time for me to send out copies of my not even close to being dated copy of an article about HASL. Though it was published in 1992, in Printed Circuit Fabrication Magazine, and it got rav

Re: bare board problem

Electronics Forum | Thu Jun 17 20:48:18 EDT 1999 | Earl Moon

| | first of all what is the technical term for the small amount of solder on a plated pad. we are getting poor screen printing gasketing on a 20 mil qfp due to this solder not being even or too high in spots and not covering the length of the pads.

Re: Poor solderability

Electronics Forum | Thu Feb 10 10:28:56 EST 2000 | Russ

Okay, Okay, here is the rest of the story! These boards were definitely plated, reworked to HASL, The component that is the most succeptable is a 160 pin QFP .5mm pitch. This component has nickel/iron lead frame. Significantly reduced apertures (1

Re: solder balling

Electronics Forum | Mon Aug 07 10:22:13 EDT 2000 | genglish

Ramon, I have had experience in the problems you are witnessing. The problem can relate to a number of factors. Obviously the printing process is the first place to start your investigations, try looking at the stencil apertures for bleed under the

Re: bare board problem

Electronics Forum | Thu Jun 17 19:40:11 EDT 1999 | Scott Cook

| first of all what is the technical term for the small amount of solder on a plated pad. we are getting poor screen printing gasketing on a 20 mil qfp due to this solder not being even or too high in spots and not covering the length of the pads. an

Re: bare board problem

Electronics Forum | Thu Jun 17 19:40:27 EDT 1999 | Scott Cook

| first of all what is the technical term for the small amount of solder on a plated pad. we are getting poor screen printing gasketing on a 20 mil qfp due to this solder not being even or too high in spots and not covering the length of the pads. an

Re: bare board problem

Electronics Forum | Thu Jun 17 19:41:29 EDT 1999 | Scott Cook

| | first of all what is the technical term for the small amount of solder on a plated pad. we are getting poor screen printing gasketing on a 20 mil qfp due to this solder not being even or too high in spots and not covering the length of the pads.

Re: bare board problem

Electronics Forum | Fri Jun 18 10:24:12 EDT 1999 | John Thorup

| first of all what is the technical term for the small amount of solder on a plated pad. we are getting poor screen printing gasketing on a 20 mil qfp due to this solder not being even or too high in spots and not covering the length of the pads. an

Re: Wavesoldering Organic Copper Coated Vias

Electronics Forum | Thu Jun 25 08:30:38 EDT 1998 | Earl Moon

| I have a single-sided board with test vias that pass through the board. The test vias are pasted and reflowed with the SMT components on the top side. When the boards are wavesoldered, the solder coverage on the vias is spotty. Some will sold

Re: Wavesoldering ENTEK PLUS Coated Vias

Electronics Forum | Thu Jun 25 09:29:01 EDT 1998 | Henry Lee

| | I have a single-sided board with test vias that pass through the board. The test vias are pasted and reflowed with the SMT components on the top side. When the boards are wavesoldered, the solder coverage on the vias is spotty. Some will so


poor hasl searches for Companies, Equipment, Machines, Suppliers & Information