Electronics Forum: poor solder (Page 1 of 92)

Alternative tin-lead solder pastes to minimize poor wetting on o

Electronics Forum | Thu Mar 22 13:06:50 EDT 2012 | smtmfgeng

Does anyone have any insight on alternatives to Indium NC-SMQ 92J solder paste for minimizing poor wetting on parts with oxidized leads (see datasheet here: http://www.dtsprocess.com/contents/articlefiles/6-SMQ92j.pdf). I am considering setting up a

Alternative tin-lead solder pastes to minimize poor wetting on o

Electronics Forum | Fri Mar 23 10:00:38 EDT 2012 | isd_jwendell

I am a big fan of AIM SnPb solder paste. I currently use NC257-2 (no-clean, 89.5%), and recommend you include it in your evaluations.

Alternative tin-lead solder pastes to minimize poor wetting on o

Electronics Forum | Fri Mar 23 03:41:19 EDT 2012 | grahamcooper22

try Almit Sn62 HM1 RMA V14L ....its the best no clean lead paste for wetting...I sell it and it has solved wetting problems many times when users have used other pastes

ENIG poor wetting

Electronics Forum | Tue Jul 30 17:47:50 EDT 2002 | davef

Dewetting: Solder does not adhere to lead or land, caused by: * Poor solderability of lands. * Poor solderability of leads. * Solder paste integrity. * Lead plating integrity. Need more information, please: * What is dewetting [ie, component, pad, e

ENIG poor wetting

Electronics Forum | Tue Jul 30 08:37:39 EDT 2002 | davef

When you talk about 'poor wetting', 'dewett', 'no wets', etc.; are you seeing solder pulling back or away from the pad? Please describe the condition. Dewetting. The condition in the solder joint in which the liquid solder has not adhered intimate

Palladium poor wetting

Electronics Forum | Tue May 23 09:50:37 EDT 2006 | flipit

They work well in silver conductive epoxy in hybrid applications. They are very poor in no clean applications. They don't work that well in OA solder paste either. Used them once in OA paste and in a nitrogen. They looked just fine. Solder to Pd

ENIG poor wetting

Electronics Forum | Wed Jul 31 17:35:16 EDT 2002 | davef

* Finally, when soldered by hand, do the problem pads take solder? Yes, the XRF analysis will be interesting.

Palladium poor wetting

Electronics Forum | Mon May 22 18:19:29 EDT 2006 | Steve

I have read some threads about poor wetting on palladium-silver (Pd-Ag) coated components. I followed the suggestions, but I am still having a problem. The part is an 0603 chip type (Vishay varistor). The Process: solder paste is lead-free Alpha Met

Palladium poor wetting

Electronics Forum | Tue May 23 09:27:37 EDT 2006 | Steve

Sorry I misled you. The PCB pads are wetting, but there is no fillet being formed. After reflow, it looks as though no paste was put down on the pads; however the paste print is fine. All other components solder real nice, it's only the Pd-Ag parts t

ENIG poor wetting

Electronics Forum | Tue Jul 30 12:15:15 EDT 2002 | Rick Lathrop

Hi Dave, The paste applied to the board ends up on the tombstone. The pad has a thin covering of solder most of the time, this is why I think they call it a dewet. Occasionally the pad shows some areas of gold and very rarely are some pads not wet at