Electronics Forum | Fri Jul 06 12:11:34 EDT 2007 | james
We are starting to see issues with using Kester WS R562 with lead free components. The joints look grainy on almost all of the 0402'2 and other small components. Some of the solder does not solder to the terminations. These are hybrid boards which
Electronics Forum | Wed Sep 18 12:35:56 EDT 2002 | stepheno
Fourth - > back to design of PCB. Are there solder dams of > mask between the pads? If yes, that helps. If > not, pay close attention to stencil aperture > width and be sure that the aperture deposits less > paste by 1-2 mils per pad, centered o
Electronics Forum | Wed Sep 18 12:31:16 EDT 2002 | dragonslayr
My suggestion is to conduct a Design For Manufacturing (DFM)study on the assembly in question. Pay particular attention to the pad sizes, component lead dimensions and satisfy yourself that those two factors are correct. Given that pads match compone
Electronics Forum | Mon Nov 09 09:44:22 EST 2015 | davef
Purpose. This describes setting-up a wave soldering system set-up for a new assembly design or checking a wave solder machine operation with a test board. Applicability. To be used for new design printed circuit assembles and during machine accept
Electronics Forum | Mon Apr 19 20:49:13 EDT 1999 | Dave F
| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185
Electronics Forum | Mon Nov 20 21:02:46 EST 2000 | Michael Psrker
First question I have for you is: Are you assuming that standard precautions are in place at your facility to minimize moisture content i.e. air- deionizers, vacuum sealed packaging, humidity control in storage and manufacturing? You do not mention
Electronics Forum | Thu Aug 13 07:53:40 EDT 1998 | Earl Moon
| | Couple of questions. | | 1) Are we talking alumina substrates as the ceramic material? | | 2) Are we co-firing gold as the conductors on the substrate surface? | | 3) In other words, is this a hybrid thick film circuit? | | 4) If so, how large or
Electronics Forum | Sat Feb 17 14:21:54 EST 2007 | Muhammad Haris
Hi All, I am using YV100Xg YAMAHA Pick and Place Mounter Machine and I am facing a tilting problem of PLCC 84 and QFP 240 pins ICs. I deeply checked about their vision files and place them on the double sided tape and found them ACCURATE on their pad
Electronics Forum | Wed Apr 21 00:35:31 EDT 1999 | Scott Cook
| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185
Electronics Forum | Thu Dec 16 15:00:20 EST 2004 | glaucon
Simple differences. Both processes require a very similar machine platform, controlled motion, vision fiducial recognition and alignment of a substrate (PCB or hybrid ceramic) to the "image", the image being either a stencil (hence stencil printing)
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830