Electronics Forum: rebake time (Page 1 of 2)

Package rebake

Electronics Forum | Wed Oct 24 02:09:34 EDT 2018 | simondsr

Hi everyone, I am new to this SMT. I have just graduated my study, have zero experience in SMT industry as I studied Automotive before. Ok lets proceed to the main objetive, I have a question regarding package rebake. From what I have learned, the

Package rebake

Electronics Forum | Fri Nov 02 19:34:19 EDT 2018 | sarason

I am assuming that your application is Automotive. The logic here is that the product has got to at least run for 8 years or more. The prebake removes any moisture that may creep into the product during the wait time. A little moisture combined with

Package rebake

Electronics Forum | Wed Jan 09 01:22:39 EST 2019 | kenneth0

Hi Simond, The baking process is likely to remove any moisture after the cleaning process. We wouldn't want any moisture trapped as this might cause delamination if the package is subject to subsequent heating/reflow process. Hence there's a staging

Baking components at 70 degree

Electronics Forum | Thu Dec 20 01:22:41 EST 2007 | gersla

As I told you, some carriers (trays) are limited to 75 degree maximum, and from time to time employees do not pay attention to this. This is one of the reasons. The second reason is that 90 degree still be problematic in a case of rebake more then 3

Baking components at 70 degree

Electronics Forum | Mon Jan 07 13:09:35 EST 2008 | stevek

As I told you, some carriers (trays) are limited > to 75 degree maximum, and from time to time > employees do not pay attention to this. This is > one of the reasons. The second reason is that 90 > degree still be problematic in a case of rebake

MSD Control

Electronics Forum | Thu Sep 22 06:54:14 EDT 2005 | Rob

Hi Gavin, Depends on what MSD class, but in general for the more sensitive parts if they've been opened & not used within the time limit it's rebake, add dessicant & seal. Our distribution side splits them down into more manageable/production size

baking out pcbs after reflow process

Electronics Forum | Thu Jul 12 11:56:20 EDT 2012 | hegemon

You might try to complete all your soldering within a 72 hour or less time frame. For all intents treat your board like a moisture sensitive component after you have baked and completed SMT reflow. Wash, blow dry, and go direct to stuffing and com

MSD Rebaking Guidelines

Electronics Forum | Fri Jul 11 13:04:13 EDT 2003 | fmonette

Hi Chris, Yes there is a limit to the bake cycles : "...the cumulative bake time at a temperature greater than 90C and up to 125C shall not exceed 48 hours. If the bake temprature is not greater than 90C, there is no limit on bake time..." Ref: J-S

Re: Help... Need new or used SOIC-16 metal tubes - Do You Really??

Electronics Forum | Tue May 05 15:45:37 EDT 1998 | Dave F

| Looking to buy used or new tubes, that will fit an SOIC-16 | Need these tubes ASAP. We need to bake these parts and drypack. | Please email or call if you can help. | Eric Jenkins | 801 956-0897 Eric I'm not sure of the manufacturer of the parts th

Re: Baking Components ?

Electronics Forum | Fri Jul 30 17:22:48 EDT 1999 | Dave F

| | Surface Mount Components like QFP's in Tray usually comes sealed in an anti-static plastic pack. In case the QFP's were removed from the said anti-static bag for more than 2 weeks, do these components needed to be baked for they might produce so

  1 2 Next

rebake time searches for Companies, Equipment, Machines, Suppliers & Information

SMT Machines

High Precision Fluid Dispensers
2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven
2024 Eptac IPC Certification Training Schedule

World's Best Reflow Oven Customizable for Unique Applications
Fully Automatic BGA Rework Station

500+ original new CF081CR CN081CR FEEDER in stock