Electronics Forum | Thu May 11 10:30:55 EDT 2017 | cyber_wolf
Does anyone know of a supplier that offers an "R" type solder paste ? Not "RMA" just "R" Thanks
Electronics Forum | Thu May 11 11:25:56 EDT 2017 | davef
Key to Rosin Fluxes [from SUPERIOR FLUX & MFG. CO.] Type R (Rosin): Non-activated rosin flux for soldering copper. Residues are non-corrosive and non-conductive. Type RMA (Rosin Mildly Activated): Mildly activated rosin flux that contains no chlori
Electronics Forum | Thu Nov 03 08:34:25 EST 2005 | Slaine
Hi We currently use a small amount of Alloy : 43Sn 43Pb 14Bi Flux: RMA-51AC, Metal : 88.5%. We use it for reworking a product and only consume about 100g per year, we are in the middle or ordering in some more paste but the MOQ is 500g. Is it possibl
Electronics Forum | Thu Feb 24 16:08:54 EST 2000 | Gary
I have the situation where we may need to use a variety of reflow temperatures. It seems that the design engineers want us to try a variety of "unspecified" pastes on the products. For example, the first PCB would be assembled using a higher temperat
Electronics Forum | Thu Feb 24 16:08:54 EST 2000 | Gary
I have the situation where we may need to use a variety of reflow temperatures. It seems that the design engineers want us to try a variety of "unspecified" pastes on the products. For example, the first PCB would be assembled using a higher temperat
Electronics Forum | Thu Mar 22 17:37:06 EST 2001 | davef
Hey!!! Watch it!!! I don�t want to get you believing too much of this stuff. But if you bought that, listen to this � some circuits are so critical with that skin effect stuff that they use silver as the top level solderability preservative. Turn
Electronics Forum | Thu Mar 22 17:38:44 EST 2001 | davef
OK, lemme take a different angle on this, �cuz I forgot to touch on this when I first responded. I mentioned a study ["Evaluation of Low Residue Soldering for Military and Commercial Applications: A Report from the Low-Residue Soldering Task Force"
Electronics Forum | Wed Mar 12 08:03:30 EST 2003 | Surachai
Hi all Pls. help advise. Our board use RMA solder paste (Pb-free Sn96.5/Ag3.0/Cu0.5). Can we use No-clean paste flux (Delta 670S1) in rework process? If it can not be used, why?. Thanks very much for your advice. Surachai
Electronics Forum | Mon Jan 24 16:37:26 EST 2000 | Kris W
To all, This may appear to be laziness on my part, but I need to ask for some advice. We are in the process of qualifying no-clean solder paste to replace or current RMA paste. I have performed qualification runs and extensive reliability testing
Electronics Forum | Fri Oct 10 14:49:21 EDT 2008 | omid_juve
what is the best solder paste type(RA,RMA,R,WS,...) for removing oxidation from the pins of our parts.