is it all right to reflow a BGA using a rework station but without applying a layer of solder paste on pcb. the diameter of the solder ball is 0.75 and the pitch is 1.5mm.

BGA rework

Electronics Forum | Tue May 14 20:58:42 EDT 2002 | davef

Maybe the issue is not a proper rework method. Your shorts on the corners are caused by too fast of a profile causing the corners of the BGA to get too hot, too fast, which made them curl, like tatter chips.

BGA rework

Electronics Forum | Wed Mar 10 00:25:36 EST 2004 | kanwal324

We have the expertise of mounting and rework of all types of bga without facing any problem. If you want or you can give us one oppurtunity. K S Walia Xo Infotech Ltd. India

BGA rework

Electronics Forum | Mon Mar 09 11:22:44 EDT 2009 | pcbrown

There are several out there. We will be doing some proprietary BGA installation in-house and I need a rework station. Has anyone had any experience with Focal Spot RD-500? Air-Vac DRS25? Or is there a better system out there for occasional to light u

BGA rework

Electronics Forum | Thu Jan 21 19:43:16 EST 1999 | Ron Costa

What are the problems related to cleaning when using OA tacky flux to replace a PBGA. Will your standard inline cleaner be able to reach all the way under to clean all residue? BGA type is 1.27mm pitch .030 dia. ball plastic. Any info helpful! Thank

BGA rework

Electronics Forum | Tue Mar 09 06:08:38 EST 2004 | Bryan

I never met such a issue.I use SRT1100&Freedom2000,and they works well with BGA larger than 3.5x3.5cm.

BGA rework

Electronics Forum | Tue Mar 09 19:40:47 EST 2004 | Vijay

The shorts happen at corner of the BGA. The PCB thickness is 1.6mm, It is a PC motherboard with all thru hole connectors mounted on.The preheating is done using IR heater and the temp is 120-160 for about 70-80 sec.I am using ERSA IR550A

BGA rework

Electronics Forum | Tue Mar 09 19:40:55 EST 2004 | Vijay

The shorts happen at corner of the BGA. The PCB thickness is 1.6mm, It is a PC motherboard with all thru hole connectors mounted on.The preheating is done using IR heater and the temp is 120-160 for about 70-80 sec.I am using ERSA IR550A

BGA rework

Electronics Forum | Fri Apr 23 03:02:46 EDT 2004 | Nick Prince

Everyones opinions will differ as to which is the best. Most people will recommend the systems they bought, fiar enough I susppose. Here is the best value system on the market, you will need to shop around. http://www.cooperhandtools.com/europe/elec

BGA rework

Electronics Forum | Thu Apr 29 18:39:11 EDT 2004 | Erhan

Hi Steven, Let me step back a bit. Have you ever removed and/or placed a QFP/BGA with a heatslug using IR before? Erhan