Electronics Forum: rosin flux 800 (Page 1 of 22)

RF 800 Flux ( cookson brand) - Flux acid calculation and restoration of acid value from 17 to 19

Electronics Forum | Fri Sep 08 12:03:24 EDT 2017 | rameshraja

Hi, I need the RF 800 Flux Acid titration procedure and also require EPT of the same to add thinner ( RF 800 additive), i.e we are using the flux rf 800 for our wave soldering process having foam fluxer , after 2 hours we are taking sample from the

Switching from full-rosin/RMA flux to no-clean flux

Electronics Forum | Mon Mar 25 21:45:22 EDT 2024 | buckeye

I got an inquiry from one of our electronics labs with regards to their soldering processes. They use eutectic (63% Sn, 37% Pb) solder. For liquid flux they are currently using Kester 186, which is an old-school, full rosin (RMA and ROL1) flux that c

Rosin versus water soluble flux

Electronics Forum | Tue Jan 02 14:12:23 EST 2001 | Dave Miller

I work for an R&D company that is starting to do some prototype and limited production circuit cards. We are deciding how we want to build these boards, and we are wondering what we should do about flux and cleaning. We have circuits that run at 15

Re: When using noclean flux or clean flux process?

Electronics Forum | Tue Sep 21 13:10:10 EDT 1999 | Dave F

| Dear All, | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | I mean that I wonder why we use

Re: When using noclean flux or clean flux process?

Electronics Forum | Wed Sep 22 02:45:23 EDT 1999 | Brian

| | Dear All, | | | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | | | I mean that I wonder

flux on PCB's after cleaning

Electronics Forum | Wed Jul 21 17:49:52 EDT 2004 | jsk

problem: Too many solvents and boards are not clean Flux remains on the board after vapor degreaser and "Powdery" white residue after vapor degreasing Flux type is kester 186 Process: hand solder High Temp alloy, spot clean after hand solder e

RMA flux Based Solder Paste

Electronics Forum | Thu Apr 05 12:25:01 EDT 2001 | davef

Talk about bucking the trend!!! OK, OK, I know some US military work still requires RMA. You�re both correct. Cleaning decisions for RMA fluxed boards are based on customers requirements. [Some do (clean) and some don�t.] Older US military speci

flux on PCB's after cleaning

Electronics Forum | Fri Jul 23 14:41:41 EDT 2004 | Steve Stach

Dear JSK, It sounds like the root causes of your problem are two fold. First, excessive heat will polymerize the abietic acid found in rosin forming neo-abietic diamers and polymers which are much less soluble than the parent monomer. There are

Removal of No-Clean flux residue

Electronics Forum | Wed Sep 05 17:37:56 EDT 2001 | seand

Hello Jeff, If you have components on your board be careful of how low the frequency is that you will be applying to your board. Ultrasonics are great for cleaning stencils and bare boards at around 40kHz. These frequencies (and Lower)may however

Cleaning OA flux with vapor degreaser

Electronics Forum | Tue Mar 09 14:53:16 EST 2010 | davef

Resistivity Of Solvent Extract [ROSE] is a bulk ion contamination [BIC] test method. It should thought of as a process control tool used to assess ionic contaminants. Don't consider it an acceptable tool for establishing 'GO-NOGO' limits. The stan

  1 2 3 4 5 6 7 8 9 10 Next

rosin flux 800 searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

We offer SMT Nozzles, feeders and spare parts globally. Find out more
Circuit Board, PCB Assembly & electronics manufacturing service provider

High Precision Fluid Dispensers
Fluid Dispensing, Staking, TIM, Solder Paste

High Throughput Reflow Oven


Best Reflow Oven


SMT & PCB Equipment - MPM, DEK, Heller, Europlacer and more...