Electronics Forum | Mon Mar 02 11:15:23 EST 2020 | slthomas
You'll want to chop your solder into "bite sized" pieces for your pot, by the way. A bolt cutter or a band saw are a couple of ways to do it without ruining other precision tools. It's up to you for the alloy you use, but there are several (some
Electronics Forum | Mon May 17 16:34:25 EDT 2004 | pjc
I am an equip mfrs rep. I took a customer to my wave solder principal's factory to run their boards on a wave with no-Pb alloy, (Sn96.5 Ag3.0 Cu0.5) in air environment. The results were excellent with pot temp of 263C (505F). Their boards are low to
Electronics Forum | Tue Feb 13 14:33:16 EST 2007 | CK the Flip
So the moral of the story is..... these SAC305 BGA's were accidentally mixed in with a Leaded process, the profile couldn't get hot enough due to Tg and Td constraints on a known good QFP on the same board, and consequently, the whole assembly fail
Electronics Forum | Mon Jun 13 07:20:10 EDT 2011 | scottp
It's more likely the warp is due to material issues. I've spent way more time than I'd care to admit running Thermoire with various profiles and there's pretty much nothing you can do to reduce warp via profile unless your current profile is truly a