Electronics Forum | Wed Oct 04 13:06:21 EDT 2006 | greg york
Sorry Bert For some reason I'm not getting the Email notifications so appologies never saw the reply. The mettalic antidrossing agent reduces the dross to levels of est. 50% less than compared to 63/37 alloy. When used with SACP/0307 alloy and SACP/
Electronics Forum | Wed May 02 04:04:18 EDT 2007 | greg york
What aload of rubbish - prove it, we have over 320 users in the UK alone using the SACP0307 solder with great results, and the biggest advantage they have is they can multiple source the solder not stuck to one company who has purchased the patent an
Electronics Forum | Tue Jan 10 14:44:42 EST 2006 | greg york
Not sure about Sn/Cu/Ni large market share here in Europe as we have a large part of the UK market with SACP0307 alloy 0.3%Ag introduced over Two years ago Also worked against Sn/Cu/Ni alloy with large TV Co and they went with 0.3%Ag due to reliabili
Electronics Forum | Wed Jan 11 18:44:42 EST 2006 | fctassembly
Hello Greg, Glad to hear your success with the SACX0307 copy. By the way, does the P mean it contains phosphorus? Does yours also contain bismuth like the SACX0307 (according to their plumbing solder patent for X0307)? In response to your discussion