Electronics Forum | Thu Jun 07 18:09:21 EDT 2007 | stephan
We noticed unsufficient soldering on some 0805 chips located between pins from a plastic bloc connector . All chips are soldered with 45� angle. Flux quantity , preheating , contact time and PCB quality was checked. Do you know any international stan
Electronics Forum | Thu Nov 15 10:33:35 EST 2007 | paulallan
Does any one know of a supplier high temperature PCB ink that can safely used between pads on an SMT connector. The product ideally should be screened on and have resistant to short exposure to heat from a selective lazer. Must be non-conductive and
Electronics Forum | Mon Dec 24 09:21:18 EST 2007 | davef
Desco sells a strap monitoring system [50430 - SMARTLOG X3, 120V, DUAL FT PL, KEYPAD, BC READER, SOFTWARE, $2861.25] that provides for using of a barcode scanner to enter employee ID. Maybe they can give you a lead on ESD safe ID cards. We have no r
Electronics Forum | Tue Feb 19 08:46:06 EST 2008 | rgduval
The last time I encountered dendrite growth, it was within a component package. I believe we were experiencing it within a crystal. The root cause was water intrusion during in line wash. The component was supposed to have been sealed and safe for
Electronics Forum | Thu Mar 20 10:57:28 EDT 2008 | patrickbruneel
In addition to Dave�s comments RE: Stands for RESIN (purified or modified rosin) No resin can be cleaned with pure DI water (requires saponification). L0: Stand for halide free activation which can safely be left on the boards. To my knowledge all
Electronics Forum | Tue Sep 09 16:00:07 EDT 2008 | ppcbs
We always bake our loaded boards before any BGA rework is done. 12 to 16 hours at 100 c. We have had incidents in the past on loaded boards where 125 c has melted parts and the occasional low temp BGA trays. 100 c has proven safe for the past 10 y
Electronics Forum | Thu Oct 30 14:26:20 EDT 2008 | davem
80 degrees F in the Summer. Also, "It is not recommended to store foods which must be kept at below 40� F for safe storage". Obviously we're not storing food, but the point is still valid. jdumont, Thanks for the data. I have a couple of Extech di
Electronics Forum | Thu May 28 16:10:07 EDT 2009 | operator
How does one keep a pcb safe from ESD when applying an aerosol conformal coating on a flat surface? Even if you had an ESD mat to place the pcb on it would quickly be coated. The only thing I can think of is an ionizer. Does not the aerosol create a
Electronics Forum | Thu Aug 20 21:52:22 EDT 2009 | davef
It's a safe bet that your solder alloys will merge and form a proper solder connection at ~230*C for 15 to 20 seconds. At process conditions with less time and temperature, it's a lot of bla-bla-bla. In order to understand the quality of the solder c
Electronics Forum | Tue Dec 27 23:16:26 EST 2011 | monicanhelp
have you tried using an ultrasonic cleaner? i heard this from a friend and told me about this option. although, you may have to use a solution with the machine. here's a link i saw before while researching on using ultrasonic cleaner for pcb: http: