Electronics Forum | Thu Feb 24 20:39:05 EST 2022 | joshsvoboda
there is evidence of wetting on the heel. This is the first time I have had this type of joint using SC100C on a leaded part. Usually there is at least some wetting on the sides instead of just looking like it is pressed in and sitting on top of the
Electronics Forum | Tue Apr 17 01:45:16 EDT 2007 | Jane
There are several alloys had been using in the industry. For SMT: most people use SAC305 For Wave: most of them use SAC305,SC100C,SCS7,and SACX0307. Of course, different alloy composition have its own recommended profile. There is no such rule tellin