Electronics Forum | Mon Jun 30 22:02:43 EDT 2003 | davef
If you don't seal your packaging, the silica gel will try to remove the moisture from the air and will become saturated pretty quickly. There is no requirement that you pack/ship with dessicants. Some customers require such things though. Why do y
Electronics Forum | Sat Jun 28 22:52:34 EDT 2003 | ramanandkini
We have an Electromechanical assembly (clock) that has a step motor on the board. This electromechanical assembly is assembled in a screw less plastic moulded casing. The plastic casing is neither air tight nor water proof. The board is with SMOBC+ H
Electronics Forum | Mon Dec 27 05:16:17 EST 2021 | jineshjpr
Hi Stephen, Thanks for your response. Since the OSP Finished PCB to be execute in mass volume, almost 3 to 4 weeks (Vacuum Sealed Pack) takes place prior to assemble. Although we are using SnPb 63-37 Type 4 solder paste for this single sided SMD asse
Electronics Forum | Thu Jun 25 09:37:48 EDT 1998 | Russ Miculich
The real causes of microcracking are not normally due to pick and place - particularly if you are using a piece of equipment with vacuum pick up and release. The real cause of microcracking is due to thermal stresses on the die and the choice of the
Electronics Forum | Fri Aug 25 07:42:29 EDT 2006 | davef
Our sympathies about the ENIG boards. B:) So, you cut the end off the barrier bag, take 200 boards, heat seal the end of the bag and restock it, build the 200 boards and ship them, right?
Electronics Forum | Mon Sep 21 15:45:35 EDT 2009 | boardhouse
Hi Ryan, Standard shelf life for FR4 Non-RoHs & Rohs material with HASL or Lead Free HASL would be 12 months + in a controlled environment. on all RoHs materials over 6 months, we would suggest your board shop run a solder ability test before ship
Electronics Forum | Fri Aug 12 22:10:24 EDT 2005 | Mika
I agree with all the prior postings! But I have some additional thoughts about this. If there is a build up of moistures (% humidity) inside the pcb; before you reflow the pcba; then you will have the result out of the oven, just as you described. My
Electronics Forum | Fri Jul 09 18:36:48 EDT 2010 | rway
We don't use flex pcbs but have the same issue here. Most of our pcbs are HASL finish. I have looked at silver and gold immersion and both look really good under my color camera on my AOI. However, gold is more pricey. There is no additional cost