Electronics Forum | Tue Oct 17 12:07:58 EDT 2006 | pms
ya don't need no stinkin pads. just run sum fine gauge insulated jumpah wires from da I.C. legs (da ones with da missin pads) to da traces or where-ever dem traces end up. dat should get er dun !!!!
Electronics Forum | Mon Mar 20 19:27:14 EST 2000 | Marc Ruggiero
Hello, I am looking for inputs (experiential or opinions) concerning field reliability of high-frequency RF boards that have had a trace or pad repair (or both), any package type. If anyone can comment on this subject, I would appreciate it. We bu
Electronics Forum | Wed Oct 17 12:46:55 EDT 2001 | rholland
Does anyone know of an IPC standard callout for testing traces and there connection to pads or vias of manufactured PCB's? I believe it should be on the Fab drawing. At this time we ask for the test on our P.O.'s. Test Voltage (XX)V Single Sides Te
Electronics Forum | Mon Feb 25 21:13:12 EST 2002 | davef
No, none of us can tell you what is the acceptable level of halide content or contamination in flux residue. The level of harmful residues on your product helps determine the reliability of your product. We know nothing of your product, its custome
Electronics Forum | Thu Sep 11 10:01:30 EDT 2014 | spoiltforchoice
1 - Too messy, parts already come in nice easy to use machine compatible packaging, tapes, reels, tubes and trays. All you are doing is adding an extra step and complication. A key production aim is to reduce the number of steps. 2 - BGA - a chip wi
Electronics Forum | Fri Apr 19 13:47:00 EDT 2019 | davef
It's a terrible idea. Through holes should be drilled in the exact center of a pad +/-. Have the two holes go out back and settle this. Whichever hole returns, that hole get to keep the pad. The other hole needs to get its own pad. End of story. Th
Electronics Forum | Wed Sep 01 14:15:27 EDT 1999 | Dave F
| Help | | I have just received some PCBs with external tracks entering SMD pads at all angles, tangents + 45 degs etc. | | Where can I obtain information as to how tracks should enter SMD pads.? I have looked at several IPC books and got some mino
Electronics Forum | Mon Mar 30 07:44:12 EST 1998 | Earl Moon
| | | | | We are having some problems with "drawbridging" on 0805 film capacitors. | | | | We have already reduced the pad width from .050" to .040" based on input | | | | from vendor. Defects appear to be random as far as location on the PWB and d
Electronics Forum | Sun Mar 29 15:42:05 EST 1998 | Michael Fogel
| | | We are having some problems with "drawbridging" on 0805 film capacitors. | | | We have already reduced the pad width from .050" to .040" based on input | | | from vendor. Defects appear to be random as far as location on the PWB and direction
Electronics Forum | Mon Nov 06 10:29:28 EST 2000 | Dean Stadem
All of the replies have merit. Here is another one. Because the cause of the tombstoning is wetting forces that are imbalanced, and one end wets faster or more readily than the other, the 0402 lifts up on that end easily because of its low mass. Incr