Electronics Forum | Wed Apr 07 08:28:41 EDT 2004 | Dougie
Hi, We are Scottish manufacturing company considering a move to Immersion Silver finished PWB's from HASL. The driver behind it being the RoHS and WEEE legislation in Europe at present. My question is... We plan on using a Sn/Cu/Ni solder bar in o
Electronics Forum | Wed Apr 07 08:30:22 EDT 2004 | Dougie
Hi, We are Scottish manufacturing company considering a move to Immersion Silver finished PWB's from HASL. The driver behind it being the RoHS and WEEE legislation in Europe at present. My question is... We plan on using a Sn/Cu/Ni solder bar in o
Electronics Forum | Thu Apr 14 06:00:01 EDT 2005 | bryan
The shelf life of immersion silver is 6 to 12 months in good storage conditions. The finish is usually coated with a protective layer that inhibits oxidation (like with copper OSP). Care must be taken when handling the boards as the protective la
Electronics Forum | Mon Apr 18 20:44:30 EDT 2005 | davef
Charly: Why do you "need to bake the PCb due to moisture issue", if you're not going to use the board? Why bake the board, just to put it back in storage, absorb moisture, and require baking again?
Electronics Forum | Wed Apr 20 01:08:16 EDT 2005 | charly
actually, i received a shipment from supplier where the vacuum seal was puntual and the HIC is out of order, the supplier ask me to bake and keep back into the store, but i worry is there any quality impact if i do so?
Electronics Forum | Fri Aug 11 14:29:58 EDT 2017 | abruno1995
I am having issues with this. I am having excess plating on my pcb board and i want to know if this is a ICP Class 1-3 Issue. 1. Excess Plating 2. Dark Vias Thank you
Electronics Forum | Fri Apr 09 20:28:14 EDT 2004 | Ken
I have experience in this. My company offers Lead free SMT and Wave soldering. I have processed ImSn, ImAg, Enig, OSP in both smt and wave. Yes, silver leaching will occur. Yes, copper leaching will occur. High tin content solders disolve everyt
Electronics Forum | Tue Apr 13 07:48:00 EDT 2004 | Dougie
Hi Ken, Our product is consumer, although our product is sold on it's reliability. We run a low volume high mix throughput. Any ideas on timescale for the Ag leaching? Sounds like it could be a safer bet to use Imm Sn boards with the Sn/Cu/Ni bar w
Electronics Forum | Tue Apr 19 11:54:36 EDT 2005 | masters
The email address was stripped from this post, a user complained about receiving a virus or some malicious code from the suspected address. Knowingly sending viral code is against the law. Posting personal information to circumvent SMTNet is again
Electronics Forum | Thu Aug 31 02:10:42 EDT 2017 | hxamalia