Electronics Forum | Fri Mar 29 10:11:02 EDT 2019 | cyber_wolf
“For a number of years now, work has been proceeding in order to bring perfection to the crudely conceived idea of a transmission that would not only supply inverse reactive current for use in unilateral phase detractors, but would also be capable of
Electronics Forum | Fri May 17 16:37:28 EDT 2002 | Tom Druan
I was wondering if anyone could direct me towards documentation on shear test methods/apparatus to test the bond integrity of a solder ball to its substrate. Thanks.
Electronics Forum | Tue Aug 27 03:45:36 EDT 2002 | seje
Hi there. We are considering to attach die chip with solder paste to the pcb at the SMD line (we are used to attach it with silver epoxy at the die bonding line before). This is a whole new method to me, so I'd like to have some opinions here. Where
Electronics Forum | Thu Nov 19 08:20:04 EST 1998 | Earl Moon
| | | | For some as yet unkown reason, we have started to have some boards sag and go under the wave. The boards are surface mount top side and conventional components wave soldered. We have checked the wave hight and both the profiles on the wave so
Electronics Forum | Thu Nov 19 09:01:00 EST 1998 | Dave F
| | | | | For some as yet unkown reason, we have started to have some boards sag and go under the wave. The boards are surface mount top side and conventional components wave soldered. We have checked the wave hight and both the profiles on the wave
Electronics Forum | Thu Nov 19 09:32:52 EST 1998 | Earl Moon
| | | | | | For some as yet unkown reason, we have started to have some boards sag and go under the wave. The boards are surface mount top side and conventional components wave soldered. We have checked the wave hight and both the profiles on the wav
Electronics Forum | Thu Nov 19 09:55:47 EST 1998 | Dave F
| | | | | | | For some as yet unkown reason, we have started to have some boards sag and go under the wave. The boards are surface mount top side and conventional components wave soldered. We have checked the wave hight and both the profiles on the w
Electronics Forum | Wed Aug 28 10:16:12 EDT 2002 | Jim M.
Sam We install a lot of die in the SMT room using same process as SMT parts.Water soluble solder paste is used for attachment of die to ceramic and boards. Biggest problem i found is the adjustment from installing the die in the bonding area. The t
Electronics Forum | Fri Apr 29 14:16:16 EDT 2011 | ppcbs
Below is the long explanation. This defect is most commonly found with BGA components, but can arrise with all components. I see it happening more now with lead free boards that are being assembled with a no clean flux. Best short term remedy is t
Electronics Forum | Fri May 13 14:08:39 EDT 2011 | eezday
This appears to be black-pad and is often the result of using specs that call for gold plating that is too thick. The black pad is corrosion that is created between the gold and electroless nickel during the gold plating process. This is counter in