Electronics Forum | Mon Jun 06 12:51:17 EDT 2016 | wlsmt
My operator applied flux gel ALPHA WS-609 on MG P/N FTH101XAP (CAP ALUM 100UF 50V 20% SMD) before aqueous washing the PCBAs. Solder paste used was ALPHA WS-820. Now the caps have yellow stains. Any solution to this is appreciated. Tks
Electronics Forum | Thu Mar 06 17:02:40 EST 2003 | Kris
Try alpha fry technologies. http://www.frymetals.com/manufacturing/solder_reclain1.html
Electronics Forum | Tue Apr 13 13:55:46 EDT 2004 | arcandspark
I have samples coming in, AIM and ALPHA, Multicore use to have manufacturing in the same town but disappeared. Your right about getting better help fro other, Indium is the worse I have ever had to deal with. They act like I am bothering them when I
Electronics Forum | Wed Apr 14 05:44:36 EDT 2004 | hun
Hi All, Just have a share with you guy. We are using T4 solder paste and also E-Stencil. We ahd try out Alpha, Kester, AIM and Qualitek. The result show Alpha had a very very heavy stack flux and can't get it clean off even by chemical
Electronics Forum | Sun Feb 27 13:42:44 EST 2005 | pmdeuel
So true, We had paste flux supplied to us from Alpha metals. It was the same as used in the solder paste. The major problem we noted was the in ability to control the ratio of paste to flux resulting in lots of voids. When we mixed enough to get the
Electronics Forum | Thu Apr 11 04:03:28 EDT 2002 | mwoodall
The Alpha metals Hi Check 500 is used to measure paste deposit thickness. The paste height is found from a micrometer reading determined by focussing a beam of light on a track adjacent to a paste deposit and then onto the solder paste. I've measure
Electronics Forum | Thu May 26 08:52:42 EDT 2011 | davef
Phil Zarrow wrote a useful paper that could help in evaluating paste. Here read it ... Evaluating Solder Paste � Not An Option Contributed by Phil Zarrow of ITM an Independent SMT consulting firm With soldering being the dominant source of assembly
Electronics Forum | Wed Oct 04 16:24:48 EDT 2006 | russ
try Alpha OM5100 this is a noclean paste that we use and have done the same thing you are now, reflowing pbfree with pb paste, we run to max temp of 230C with this paste and use a straight ramp with no soak profile is about 4 mins long from ambiant
Electronics Forum | Fri Feb 23 09:55:02 EST 2024 | carl_p
Got you. 225C for peak does seem low to me. Henkle is the main one i've used with a peak of 245c & Alpha around the same although I try to keep that at no higher than 235C as we use it for LED arrays. If the peak is that low, is the liquidus te
Electronics Forum | Fri Aug 01 12:35:54 EDT 2003 | blnorman