Electronics Forum: solder problem (Page 224 of 507)

Re: Solder Paste

Electronics Forum | Wed Jan 13 21:46:03 EST 1999 | Dave F

| I am currently using Alpha WS629. I have a Malcom SPS-1 Solder paste mixer. I find that the mixer after running for the recommended mixing time | (10 to 18 Min) ball's the solder in the jar. | | 1) Is there any other Manufacture having the same

Component Skew during Reflow Process

Electronics Forum | Tue Nov 05 10:55:41 EST 2019 | engmagana

Hi Ameen, Did you fix it? I had the exact same problem with the same type of coil , check the images , LF solder SAC305, we have adjusted the solder apertures to the minimum solder required to have a strong joint enough to break the pad from the bo

DFM Guidelines

Electronics Forum | Wed Aug 12 00:01:56 EDT 1998 | Peter

I have a customer who is transitioning from 100% thru hole boards to designing boards with smt components. We gave them our basic DFM guidelines and they have laid out 2 boards following these guidelines. When I saw the result of their first pass, I

Re: Ferrite Bead 1206

Electronics Forum | Tue Nov 02 11:44:54 EST 1999 | Wolfgang Busko

Hi Pat, is the soldering Ok when you solder them by hand ? We use some larger ferrite beads with no problems in reflow but I must say that we use a vapour phase and only max 5 parts/PCB. They do have a high thermal capacity and you use a lot of them,

Hybrid reflow profiles

Electronics Forum | Sat Oct 01 01:04:47 EDT 2005 | ck

I face a problem where the components termination is non lead free but solder alloy is lead free. Thus i am using hybrid reflow profile. The specs for the reflow profile i am using: reflow temp. 120 to 160 deg C; time 90 to 120 sec. As for the pak te

Solder balls

Electronics Forum | Fri Nov 15 00:08:01 EST 2019 | ramesh_10377

hi i recommend following actions. 1) check the location where most solder ball is finding 2) verify the printer setting parameter if the problem is still persisting please go below action 1. Stencil thickness should be 4 mil 2. Aperture ope

Re: En-Tek Coating

Electronics Forum | Tue Oct 06 17:17:44 EDT 1998 | Chrys

| We are experiencing poor wetting on various components placed on a PCB with En-Tek coating. Is anyone else experiencing simular problems ? We have the following questions: | | 1. How can the thickness of the En-tek coating be measured? | 2. Is En

Re: Hand Lotions For Operators

Electronics Forum | Wed Jun 10 23:26:09 EDT 1998 | Steve Gregory

| We use them, but we never thought about them. | WHAT ARE THEY? The hand lotion we provide for our operators. | BACKGROUND: Operators hands take a beating. They | 1 Work in a humidity controlled 35 to 50%RH environment that is drying | 2 Wash b

Re: Hand Lotions For Operators/Yes But ...

Electronics Forum | Thu Jun 11 09:09:12 EDT 1998 | Dave F

| | | We use them, but we never thought about them. | | WHAT ARE THEY? The hand lotion we provide for our operators. | | BACKGROUND: Operators hands take a beating. They | | 1 Work in a humidity controlled 35 to 50%RH environment that is drying

Re: Hand Lotions For Operators

Electronics Forum | Thu Jun 11 09:05:50 EDT 1998 | Earl Moon

| | | We use them, but we never thought about them. | | WHAT ARE THEY? The hand lotion we provide for our operators. | | BACKGROUND: Operators hands take a beating. They | | 1 Work in a humidity controlled 35 to 50%RH environment that is drying


solder problem searches for Companies, Equipment, Machines, Suppliers & Information