Electronics Forum | Tue Oct 26 08:41:56 EDT 2004 | Bob R.
When we first got into BGAs on ENIG we were getting joint cracking at in-circuit test. The joints were breaking in the Sn-Ni intermetallic. We did a lot of pull testing while working with our board suppliers and our conclusion was that pull testing
Electronics Forum | Wed Jun 26 08:54:53 EDT 2002 | davef
it has a lousy gage. * Solderability testing machines from different suppliers produce dissimilar results. * Tests don�t well represent in-use. For instance, how does one test the solderability of a BGA? [Ooo, ooo. I know the answer. => For BGA and