Electronics Forum | Fri Sep 12 08:01:55 EDT 2008 | davef
There is no standard. On the web, you can find shelf life estimates for various types of solderability protection on bare boards. These estimates won't translate directly to the storage of assembled boards, because assembled boards [and the solderabi
Electronics Forum | Sun Aug 08 20:59:55 EDT 1999 | Dreamsniper
| | | What oven temperature should be used to reflow solder (Sn63Pb37) on a PC board (0.075" to 0.100" thickness) in 5 to 10 minutes? | | | | Profiling - tedious but important. As said, start with the paste manufacturers recomendation which is usua
Electronics Forum | Wed Nov 28 22:33:24 EST 2007 | davef
There is no specification for lead-free HASL. You can use any lead-free solderability protection that meets your customer requirements. Use IPC-9701 �Performance Test Methods and Qualification Requirements for Surface Mount Solder Attachments� to ass
Electronics Forum | Wed Nov 01 07:32:33 EST 2006 | davef
What you have run up against is the unfortunate consequence of the transition period from Sn-Pb to Pb-free. In the past 2-3 years there have been several studies highlighting the differences in reliability between mixed metal systems, Sn/Pb, and SAC
Electronics Forum | Tue Jun 18 04:01:07 EDT 2019 | aite
Hi! You can choose low-temperature solder paste. The low-temperature solder paste is tin and antimony with a melting point of 138 °C. When the components of the patch cannot withstand the temperature of 200 ° C and above and the patch reflow process
Electronics Forum | Mon Jan 04 22:59:23 EST 1999 | Kris Ewen
I'd like to add something about the ECD product. During a past work term (I'm a a co-op student) in an SMA plant, I worked extensively with the Super MOLE Gold in developing the reflow profiles for high-mix, low-volume production. I was 'married' t
1 |