Electronics Forum | Wed Jun 25 18:17:48 EDT 2003 | Brian W.
Water soluble pastes generally work best with a ramp-to-spike reflow profile. Check your paste manufacturer's recommended profile. There are many factors that impact your profile; board thickness, component density, buried thermal masses, board si
Electronics Forum | Tue Nov 07 09:25:36 EST 2006 | pjc
Can be done with AquaStorm 200, with some mods. I worked on a project a few years ago for a military company that needed to clean no-clean solderpaste residues from under LCC devices, we're talking like 2mil standoff. We ended up using a Zestron clea
Electronics Forum | Fri Feb 28 10:32:45 EST 2003 | pjc
Cookson Electronics Equipment- Electrovert AquaStorm 200 highly recommended options: Checkmate Conveyor Hurricane Jets in Wash and Rinse 4 Additional Top Spray Bars in Wash *Closed Loop Filtration System for Wash *Positive Displacement Chemical Meter
Electronics Forum | Thu Sep 05 18:15:15 EDT 2002 | pjc
There are chemistries out there that will solublize some post-solder NC flux residues. I have had success with Zestron material Vigon A200 and Petroferm material Hydrex DX. Go to http://www.zestron.com and http://www.petroferm.com These are chemical
Electronics Forum | Fri Dec 08 21:26:44 EST 2006 | billwestiet
You already have some good answers. A chemical isolation zone for RMA is a good idea. If you are looking for new see the two references you have and Austin America. If you are looking for used, see us at http://www.ietechnology.net. We presently
Electronics Forum | Sun Feb 05 17:44:47 EST 2017 | spoiltforchoice
Printer->Paste Inspection(which might be a feature of the printer)->High speed placer (for all the little parts)->Accurate Placer(for your BGA Processor,RAM,eMMC and big things that don't fit in the high speed)->Reflow oven->AOI->PCB stacker All of t