Re: Cleaning procedures for Entek-Plus Cu-106A

Electronics Forum | Sun Apr 25 12:01:58 EDT 1999 | Earl Moon

| Earl said, in essence: | | | Justin is absolutely right ... | | | | Again, Entek is not much more than a flux coating ... | | | | Metallic coatings protect best, as we all know - especially those electroplated. Those coatings chemical come in ne

Re: What is spec on stretch????

Electronics Forum | Mon Apr 19 10:14:12 EDT 1999 | Justin Medernach

| | | Hi, | | | I just cheesed my previous attempt at this. I looked through IPC 600 and couldn't find anything relating to dimensional stability of a board with regard to stretch. I found bow and twist but nothing on size. I have a PCB that is .0

Re: Discoloring of Soldermask and silkscreen

Electronics Forum | Mon Apr 19 20:49:13 EDT 1999 | Dave F

| Netters, | | When I reflow a PCB there is a discoloration of silkscreen and mask. It appears if Profile is too hot! But I dont think so, maybe I'm wrong? | | 1. Kester 293 no clean | 2. 2.1 C/s for 30s to 150 C | 3. .5 - .7 C/s for 60s to 185

Re: BENT LEADS ON FINE PITCH

Electronics Forum | Tue Apr 13 04:54:53 EDT 1999 | Charles Stringer

| | DOES ANY ONE KNOW HOW I CAN STRAIGHTEN | | BENT PINS ON A FINE PITCH QFP WITH OUT DAMAGING | | THE CHIP. AT $300 A CHIP I CAN'T SCRAP THEM. | | | I use tweezers and picks. I place the component down on it's backside (legs up) and manually twe

Re: BENT LEADS ON FINE PITCH

Electronics Forum | Tue Apr 13 12:36:57 EDT 1999 | Scott McKee

| | | DOES ANY ONE KNOW HOW I CAN STRAIGHTEN | | | BENT PINS ON A FINE PITCH QFP WITH OUT DAMAGING | | | THE CHIP. AT $300 A CHIP I CAN'T SCRAP THEM. | | | | | I use tweezers and picks. I place the component down on it's backside (legs up) and ma

Re: Choosing a spray fluxer.

Electronics Forum | Thu Apr 08 13:24:36 EDT 1999 | ADRIANO FERNANDES

| | I am getting ready to purchase a spray fluxing system for a no-clean process. I have narrowed it down to the Nordson or Dover system. Does anyone have any experience with either. If so can you relate with me. I am a little leary of the Nordso

Re: Intrusive soldering

Electronics Forum | Tue Mar 23 04:07:44 EST 1999 | Scott Davies

Rob, We are also using intrusive reflow to simultaneously process SMT and Thru-hole components. Our arrangement goes as follows: - Screen print solder paste to the single sided PCB using 0.008" laser cut stencil. - Apply adhesive dots to selected

Re: Intrusive soldering

Electronics Forum | Thu Mar 25 14:00:45 EST 1999 | Bob Willis

| Rob, | | We are also using intrusive reflow to simultaneously process SMT and Thru-hole components. Our arrangement goes as follows: | | - Screen print solder paste to the single sided PCB using 0.008" laser cut stencil. | - Apply adhesive dots

Re: Chip Resistor Failure

Electronics Forum | Wed Mar 24 02:23:14 EST 1999 | P.L. Sorenson - Technical Consultant

| | | Has any one seen failures of chip resistors after 1-2 years where the junction between the silver termination and the restive element on the top of the ceramic has corroded through. This results in a high resistance failure after this period of

Re: Chip Resistor Failure

Electronics Forum | Thu Mar 25 02:22:32 EST 1999 | P.L. Sorenson - Technical Consultant

| | | Your problem may be related to silver migration (leaching) into the solder. I had what seems to be a similar problem. The solution was using solder with 2% silver content. See these pages for a bit more information: | | | | http://www.ferr