Electronics Forum: used and equipment (Page 86 of 405)

SOT23s and paste + glue

Electronics Forum | Mon Dec 22 14:52:18 EST 2008 | wrongway

We run our process like that all the time paste then glue we use same profile as if we were just reflowing paste once in a while we have A plastic bodied part that has that problem we asume it was some mold relase still on the part basicly comtamena

Ecofree 303 conductive and corrosive?

Electronics Forum | Mon Aug 24 06:12:31 EDT 2009 | ghepo

joanne please pay attention, each heavy no-clean flux residues not completely heated due to hand soldering becomes a moisture absorbing conductive pathway, causing electrical leakage. So I suggest you to clean well the board after hand soldering or

UIC GSM and NiPdAu pads

Electronics Forum | Mon Oct 19 15:43:37 EDT 2009 | dilogic

We have a problem with QFN IC's with NiPdAu plated pads. Our ULC's don't see the pads due to the almost ideal reflection. Vision sees the pads almost black. As we don't have OAL-cameras (which can help in this case, I assume), I am thinking of back-l

Easy and inexepnsive SMT machine?

Electronics Forum | Wed Mar 23 19:57:18 EDT 2011 | dlou87

Im sure this has been gone over before, but what the heck! We are mounting LEDs on metal core PCBs. Almost all of them have domes of silicone on top. We have some large boards (largest is 2ft x 3") Not concerned with parts/hour or fancy features.

01005 components and reflow profiles

Electronics Forum | Mon Apr 09 20:55:46 EDT 2012 | action_101

I forgot to add that we are using a 3 mil stencil. It seems like to me that may be there isn't enough flux left when we reach liquidous?? About half of the solder spheres do melt and wet on each pad, but the top half of each solder joint is just the

Manual Pick and Place Manuals

Electronics Forum | Sat Sep 15 00:22:41 EDT 2012 | sarason

The first one I found on Google images. Just a strait search http://www.google.com.au/search?q=Model+SMT-8000&ie=utf-8&oe=utf-8&aq=t&rls=org.mozilla:en-US:official&client=firefox-a Third item down. I used to own a near identical model except tat it h

paste Sn42/Bi58 and Lead Finish

Electronics Forum | Fri Nov 02 14:46:18 EDT 2012 | ericrr

So how does this (lead free paste Sn42/Bi58) solder compare with the Sn-Ag-Cu (Tin-Silver-Copper) combination which does not flow as well (in the oven), needs higher oven temperature, (that can be adjusted by reducing the oven chain speed) and cost m

seperation of soldermask and pcb

Electronics Forum | Tue Mar 25 13:55:05 EDT 2014 | horchak

Ok lets put it this way. If the PCB house used a high quality mask and properly applied it to a properly cleaned surface and properly cured it, then as Dave stated above there are only two things that can destroy it. Excessive heat and overly aggress

Component Database and Placement List

Electronics Forum | Mon Oct 23 02:37:02 EDT 2017 | directx995

Hello, I'm looking for a friendly suggestions or best practices for creating Component Database. For example how do you discern different types of SOIC8, with different body size and pitch between leads? How do you categorize and name components? An

MPM Accuflex questions and issues

Electronics Forum | Sat Feb 10 10:08:04 EST 2018 | griinder

We recently acquired used MPM Accuflex. Immediately I noticed the live vision is mirrored. This makes it incredibly difficult to teach fiducials. I noticed some smudges on the lens, which leads me to believe the camera assembly was "worked on" at som