Electronics Forum: vapor reflow (Page 1 of 18)

vapor phase reflow

Electronics Forum | Wed Nov 17 09:28:40 EST 1999 | Steve Z

Hello, I am new to the SMT area and I need to know what a "good" vapor phase reflow profile should look like. The fluids we are using have a BP of 45 C and 219 C. Thanks,

Re: vapor phase reflow

Electronics Forum | Fri Nov 19 05:12:21 EST 1999 | Graham Naisbitt

Steve, If you can get me your snail-mail address, I will send you some latest information. We actually have a totally new system called Delta 5. It is Condensation Soldering rather than Vapour phase, the difference being that we solder in an air ti

Pb free vapor soldering

Electronics Forum | Thu Dec 22 15:36:03 EST 2005 | CC

In general two step temperature reflow process requires minimum 40 deg C delta to be sucessful. We are not using vapor phase soldering but we have similar situation when we change to SAC lead free solder for PCB component population and secondary swe

Pb free vapor soldering

Electronics Forum | Thu Dec 22 12:05:37 EST 2005 | Tony

Currently we are using a 2 step vapor soldering process to manufacture our std. lead soldered parts. The first step was done with a ls240 vapor fluid and the second was done with a ls200 fluid. Using a 221 deg C sn95/Ag5 solder for the first step a

Re: BGAs and vapor phase

Electronics Forum | Mon Jul 19 12:37:15 EDT 1999 | Wolfgang Busko

| | | | | Hi, SMTASSY | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | First, we do not do real series produktion, only prototyping up to som

Re: BGAs and vapor phase

Electronics Forum | Tue Jul 20 05:29:14 EDT 1999 | Wolfgang Busko

| | | | | | | | Hi, SMTASSY | | | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | | First, we do not do real series produktion, only prototypi

Vibrating reflow

Electronics Forum | Wed Sep 17 04:15:23 EDT 2003 | C Miller

The magnetic thing from the sot23 thread made me think of somthing from the past. Does anyone have any experience with vibrating boards during reflow? I know for a fact that if you vibrate a board during reflow it will alow the parts to "float" and

Multiple reflow cycles

Electronics Forum | Fri Mar 21 20:21:41 EST 2003 | Grant

Hi, I can verify that, and we have done 2 or more reflows with prototypes, using vapor phase reflow, and because there is no oxygen, the result is good, and you cannot tell the difference between the first reflow, and the 3rd. We are getting a vap

Multiple reflow cycles

Electronics Forum | Wed Mar 19 20:40:27 EST 2003 | arminski

Vapor Phase process can do reflow from 4 to 5 times!

vapour phase reflow soldering technology

Electronics Forum | Wed Jan 30 12:37:49 EST 2002 | jax

nifhail, In a nutshell: Vapor-phase reflow is a process that uses a fluid with a selected boiling point. As condensation of the hot vapor occurs on a cool assembly the assembly's temperature is rapidly raised to match the temperature of the vapor.