Electronics Forum | Tue May 26 06:56:40 EDT 2009 | xinxi
Hi! From your post, it seem like the wave did not really touch the component. You probably need to get the both wave height correct and that it hits the component.It is normal for solder to come through the PCB when using chip wave. The through-hole
Electronics Forum | Fri May 29 02:08:08 EDT 2009 | cobar
Check that you are getting an even spray pattern from the fluxer.Check that the chip wave nozzle is clean and if possible feed the PCB in to the wavesolder unit at 90 � or 180�.
Electronics Forum | Mon May 25 21:10:28 EDT 2009 | padawanlinuxero
Hello !! I have a problem with my wave solder oven, in one of the products we made has connectors on one side of the pcb and in the other one has SMT components the process is kinda tricky on the SMT components we use an adhesive and put to the refl
Electronics Forum | Sat Aug 26 12:26:57 EDT 2000 | Ramon I Garcia C
Hi friends: I have a problem in the process of one PCB, I have a lot of insuficients of solder in top of the board, this pcb already was working good, but sudenly began there isn't flow thru hole, I ran the profile and it was ok, if I inmerse i
Electronics Forum | Mon May 29 23:39:11 EDT 2006 | Faizal
Can anyone advice me on the effect of SN100C wave solder on SAC305 hasl board? I suppose the silver content on the hasl pcb would leech(contaminate) into solder pot.? Would it affect the surface bonding between copper pad and the solder.?
Electronics Forum | Wed Jun 13 06:42:14 EDT 2012 | brettrenishaw
We have a problem with our Unleaded wave solder machine only randomly soldering some pads. I have looked at the flux level and that appears fine aswell as cheking the preheat and solder height in the bath. The probelm is not exclusive to one perticul
Electronics Forum | Thu Jun 14 04:24:32 EDT 2012 | brettrenishaw
Yes pads are still gold after the wave soldering process even if you wave solder a pcb several times. I have tried soldering using an iron and the solder takes to the pad as you would expect. This happens on all boards of this type and all boards are
Electronics Forum | Fri Jun 22 06:31:08 EDT 2012 | grahamcooper22
Are you spray fluxing ? If so, check that you are getting flux onto the whole pcb uniformly.... That BLT flux is a water based material, are you getting rid of all the water in the preheat before you get to the wave ( can you hear any spitting as t
Electronics Forum | Mon Aug 28 15:34:19 EDT 2000 | Steve Harshbarger
Hello Ramon, This is a very common problem that usually can be overcome. Can you tell me the flux type you are using (manufacturer, and flux number)? Has your board vendor, or type of PCB's changed (are they entec coated - bare copper)? What is t
Electronics Forum | Mon Jun 18 04:21:22 EDT 2012 | brettrenishaw
Measured the pot temprature independantly from the software (268C/514F from moving wave). We are using Dross Inhibiter Tin/P Regenerator from BLT. Monthly sample checks are carried out on the solder bath and are all within limits. It will be hard to
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830