Electronics Forum | Tue Oct 12 05:09:13 EDT 1999 | Brian
| | | | | | | Can anyone tell me the formula/method to determine | | | | | | | the amount of weight that solder's surface tension can support. | | | | | | | (ie: Maximum weight of components soldered onto a bottom side | | | | | | | of a board during
Electronics Forum | Sat Oct 09 04:17:21 EDT 1999 | Brian
| Can anyone tell me the formula/method to determine | the amount of weight that solder's surface tension can support. | (ie: Maximum weight of components soldered onto a bottom side | of a board during a top side reflow on a Paste/Paste process). |
Electronics Forum | Sat Oct 09 07:33:23 EDT 1999 | Dave F
| | Can anyone tell me the formula/method to determine | | the amount of weight that solder's surface tension can support. | | (ie: Maximum weight of components soldered onto a bottom side | | of a board during a top side reflow on a Paste/Paste proc
Electronics Forum | Sat Oct 09 09:18:21 EDT 1999 | Dave F
| | | | Can anyone tell me the formula/method to determine | | | | the amount of weight that solder's surface tension can support. | | | | (ie: Maximum weight of components soldered onto a bottom side | | | | of a board during a top side reflow on a
Electronics Forum | Mon Oct 11 12:49:11 EDT 1999 | John Thorup
| | | | | | Can anyone tell me the formula/method to determine | | | | | | the amount of weight that solder's surface tension can support. | | | | | | (ie: Maximum weight of components soldered onto a bottom side | | | | | | of a board during a top s
Electronics Forum | Sat Oct 09 09:07:48 EDT 1999 | Brian
| | | Can anyone tell me the formula/method to determine | | | the amount of weight that solder's surface tension can support. | | | (ie: Maximum weight of components soldered onto a bottom side | | | of a board during a top side reflow on a Paste/Pa
Electronics Forum | Sat Oct 09 10:30:24 EDT 1999 | bix
| | | | | Can anyone tell me the formula/method to determine | | | | | the amount of weight that solder's surface tension can support. | | | | | (ie: Maximum weight of components soldered onto a bottom side | | | | | of a board during a top side refl
Electronics Forum | Fri Feb 17 11:01:47 EST 2006 | amol_kane
with lead-free solders, one would expect to find less instances of tombstoning. this is because SAC alloys are not eutectic and melt over a range of temp (usually 217-220 deg C) instead of at a single temperature. therefore the forces due to solder s
Electronics Forum | Thu Oct 05 11:40:49 EDT 2006 | Mario Scalzo, SMT CPE
David, We have seeing this more and more in the recent weeks. In a nut shell, yes; we believe that the voids that you are seeing are from the trapped air in the via from printing over it. If you could remove the Kapton tape, this might help. Also
Electronics Forum | Sat Mar 21 12:19:51 EST 1998 | David Pick
I have read somewhere of a ratio of component weight vs. surace contact area rule for double reflow soldering. This ratio is the maximum weight vs. surface tension to hold a component on during the second reflow. With this number, a person could weig
The SMTA membership is a network of professionals who build skills, share practical experience and develop solutions in electronic assembly technologies and related business operations.
Training Provider / Events Organizer / Association / Non-Profit
6600 City W Pkwy
Eden Prairie, MN USA
Phone: 952-920-7682