My guess is that he is talking about the gold plated pads not fully wetting with solder. We have seen this on some of our ENIG boards with the gold still showing at the far corners of the rectangular pads. Not knowing if this is hand soldering or p

seperation of soldermask and pcb

Electronics Forum | Tue Mar 25 11:25:18 EDT 2014 | horchak

The first impression I get is that the mask was applied over dirty or contaminated copper. What is the trace and land finish on the PCB? You also appear to have a wetting problem.

seperation of soldermask and pcb

Electronics Forum | Tue Mar 25 13:55:05 EDT 2014 | horchak

Ok lets put it this way. If the PCB house used a high quality mask and properly applied it to a properly cleaned surface and properly cured it, then as Dave stated above there are only two things that can destroy it. Excessive heat and overly aggress

seperation of soldermask and pcb

Electronics Forum | Tue Mar 25 11:43:48 EDT 2014 | sara_pcb

It is Solder Mask on Bare copper, The land finish is HASL as per MIL-PRF-55110G which accepts trace of HASL as acceptable. Wetting is acceptable. regards, R.Saravanan

Voids - correlation with a not wetting PCB

Electronics Forum | Sun Oct 11 13:53:26 EDT 1998 | Vincenzo Longobardo

I have datas to substain that a not wetting PCB ( the HAL oxided or not uniform in thickness )if soldered in reflow, it shows voids with X-Ray inspection.The voids are in side all the joints not only on the solder pads levell. Is there a technical d

Solder wetting test for PCB's

Electronics Forum | Mon Apr 23 14:02:26 EDT 2001 | relensky

I am looking for a repeatble method to determine the quality of solder wetting to a PCB. I would like something that I can perform in-house, at low cost, with reliable results. My goal is to test the wetting on white-tin PCB's, after repeated reflo

Re: Voids - correlation with a not wetting PCB

Electronics Forum | Tue Oct 13 18:32:35 EDT 1998 | Vincenzo Longobardo

Dear Mr. Earl Moon please give me all your information and pictures to know the reason of the voids formation caused by the HASL oxidation. I am very interested to this experience. With Best Regards V.Longobardo |

Solder wetting test for PCB's

Electronics Forum | Tue Apr 24 11:48:06 EDT 2001 | relensky

Thank you for the input

Non wetting spots of flex PCB pads

Electronics Forum | Thu Jun 29 09:55:54 EDT 2023 | matouschekd

Yes, i tried cleaning it with PCB-Cleaner. Sadly, no success

Re: Voids - correlation with a not wetting PCB

Electronics Forum | Wed Oct 14 08:32:45 EDT 1998 | Earl Moon

| Dear Mr. Earl Moon | please give me all your information and pictures to know the reason of the voids formation caused by the HASL oxidation. | I am very interested to this experience. | | With Best Regards | V.Longobardo | | | | I will assemble

  1 2 3 4 5 6 7 8 9 10 Next

wet pcb searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830

SMT feeders

High Precision Fluid Dispensers
Electronic Solutions

Stencil Printing 101 Training Course
Software for SMT

Best Reflow Oven