Electronics Forum | Mon Aug 22 11:50:02 EDT 2011 | rway
Yes, but even high force probes are not a cure-all. You still get flux build-up over time which can cause contact issues. The best way is to use a low residue flux in the wave to minimize what's left on the pcb post-wave.
Electronics Forum | Thu Apr 08 10:11:27 EDT 2004 | Dreamsniper
Hi Guys, Have you tried using a standard dish washer for cleaning PCB's with BGA's. What detergent or cleaning chemicals did you used? I wonder if it will work to clean a WS Flux PCB using the dish washer then get it rinsed by an old aqueou cleaner
Electronics Forum | Wed Dec 19 01:17:13 EST 2001 | ianchan
Hi Experts, I need help here, advice appreciated from all... Production is running a Lot of flex-circuit PCB, through the SMT line, with 0402 components. The flex-PCB is taped to FR4 support "pallets" when processing thru' the SMT P&P m/c. We use
Electronics Forum | Mon Mar 09 14:16:37 EDT 2020 | oxygensmd
I used to work with S15/F3, was a 10 years ago. 1. Test your machine controllers and station controllers. Load the last program with actuell command. 2. You can check what happening in the SiPlace, switch the monitor to MC, let see all bootup perfec
Electronics Forum | Mon May 31 15:09:56 EDT 1999 | JohnW
| | | | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processi
Electronics Forum | Mon May 31 15:10:14 EDT 1999 | JohnW
| | | | | | | | I have always thought it to be a good practice to wash SMA's with water soluble paste (WS609) soon after reflow. Is there a time limit as to how long a board should sit after reflow before washing said board? For instance; processi
Electronics Forum | Mon Jul 26 13:15:51 EDT 1999 | jseagle
I guess I wasn't too specific. We currently use 1,1,1 for spot cleaning and minimal rework of PCBs. If there is a lot of rework on a PCB we will use water soluble flux and wash it. This may turn out to be our only alternative, but I hate washing a
Electronics Forum | Tue Apr 13 19:14:25 EDT 2004 | Dreamsniper
Hi DaveF, To explain. The BGA that we have is from Motorola. The solder balls of these BGA's are Eutectic Solder and processed using a NC flux (as per info from supplier). So this means that the BGA pad and solder connections had NC flux process. W
Electronics Forum | Mon Jul 26 16:50:12 EDT 1999 | Bill Schreiber
If you were cleaning pallets, BTU air amplifiers or other tooling, I could provide some recomendations. However, we are not involved with the post solder cleaning of PCBs. Sorry. Regards, Bill Schreiber | I guess I wasn't too specific. We current
Electronics Forum | Tue Feb 07 11:55:27 EST 2023 | tommy_magyar
What I would look at is the chemicals being used in the facility where the complaints are. Flux/flux gel, IPA, cleaning agents, etc. Perhaps you should limit the usage to certain people only, who would be trained how to properly use these. Something
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830