Hi all How can I clean the white residue between QFP 0.5 mil Pitch? The white residue was created from mistake adding liquild No-clean flux Lonco 23F for reworking clean board. I can clean almost of it by using EC7M cleaning solvent except between
Electronics Forum | Wed Jan 27 19:42:34 EST 1999 | parag palshikar
i am working with the noclean process and getting white residues on the bottomside of the board probably due to the wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated temperature a
Electronics Forum | Thu Jan 28 08:42:43 EST 1999 | Dave F
| i am working with the noclean process and getting white residues on the bottomside of the board probably due to the | wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated temperatu
Electronics Forum | Wed Jan 27 21:02:53 EST 1999 | Dave F
| i am working with the noclean process and getting white residues on the bottomside of the board probably due to the | wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated temperatu
Electronics Forum | Thu Jan 28 08:58:10 EST 1999 | Peet
| | i am working with the noclean process and getting white residues on the bottomside of the board probably due to the | | wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated tempe
Electronics Forum | Fri Apr 03 02:52:42 EST 1998 | Jacqueline Coia
At this moment in time we are using water soluble solder paste on our PCBs these are cleaned using water only, agitated with ultrasonics. After drying a white/grey residue is left around solder joints. Reflow profile is fine and a reliable wash proce
Electronics Forum | Wed Jan 27 23:29:28 EST 1999 | parag palshikar
| | i am working with the noclean process and getting white residues on the bottomside of the board probably due to the | | wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated tempe
Electronics Forum | Thu Jan 28 09:45:44 EST 1999 | parag
| | i am working with the noclean process and getting white residues on the bottomside of the board probably due to the | | wave soldering flux.i am using a no-clean solder paste and a noclean wave solder flux.The boards passed the accelerated tempe
Electronics Forum | Fri Jan 29 05:14:06 EST 1999 | Graham Naisbitt
Hi guys, I really am at a loss to understand this one. It would appear that there may be some reaction between the flux and the resist? Or maybe you have an OSP on the board that is reacting during soldering? As a fast fix, maybe you should try a
Electronics Forum | Wed Feb 10 12:52:21 EST 1999 | Dick Casagrande
|I'm getting in a little late on this but my 2 cents is: We have been using no-clean flux for a few years now but up till last month were still cleaning (the white residue) our boards (all thru hole). Finally did some investigation and found the flux