Partner Websites: enig flash gold (Page 1 of 5)

Gold Wire Bond Failing Pull Test - EPTAC - Train. Work Smarter. Succeed

| https://www.eptac.com/ask/gold-wire-bond-failing-pull-test/

? Did the wire break at the weld? Did the plating come off the board? We need to define what kind of gold plating is on the board. Is it Electroplated Gold? Is it ENIG

Failing to Remove Gold Plating in Final Assembly - EPTAC - Train. Work Smarter. Succeed

| https://www.eptac.com/faqs/ask-helena-leo/ask/failing-to-remove-gold-plating-in-final-assembly

board’s acceptance in final assembly? Answer: The gold plating on boards is typically an ENIG coating, which is Electroless Nickell, Immersion Gold plating

Failing to Remove Gold Plating in Final Assembly - EPTAC - Train. Work Smarter. Succeed

| https://www.eptac.com/ask/failing-to-remove-gold-plating-in-final-assembly/

board’s acceptance in final assembly? Answer: The gold plating on boards is typically an ENIG coating, which is Electroless Nickell, Immersion Gold plating

PCB Assembly Technology Roadmap | Imagineering

Imagineering, Inc. | https://www.pcbnet.com/capabilities/assembly/technology-roadmap/

• Inner Layer - 10 oz • Inner Layer - 16 oz Buried/Blind Via 10+N+10 (HDI) Plasma Desmear Yes Outline Tolerance +/-.004 Surface Finish • HASL • ENIG • Immersion Silver • OSP (ENTEK) • Carbon • Immersion Tin • Electrolyic Gold • ENEPIG • ENIPIG Impeadance Control

Imagineering, Inc.

PCB Fabrication Technology Roadmap | Imagineering

Imagineering, Inc. | https://www.pcbnet.com/capabilities/fabrication/technology-roadmap/

• Inner Layer - 10 oz • Inner Layer - 16 oz Buried/Blind Via 10+N+10 (HDI) Plasma Desmear Yes Outline Tolerance +/-.004 Surface Finish • HASL • ENIG • Immersion Silver • OSP (ENTEK) • Carbon • Immersion Tin • Electrolyic Gold • ENEPIG • ENIPIG Impeadance Control

Imagineering, Inc.

Tempered Leads, Class 3 Rework, Toe Fillets and More | EPTAC

| https://www.eptac.com/webinar/tempered-leads-class-3-rework-toe-fillets-and-more/

. Definition of Class III Rework. Dissecting Toe Fillets on Gull Wing components. Understanding Gold Plating vs. Gold Flash. Course Length: 47 Minutes Cost: FREE Presenter(s): Leo Lambert Download PDF Presentation Watch On Demand More Webinars Flux Classification

Tempered Leads, Class 3 Rework, Toe Fillets and More - EPTAC - Train. Work Smarter. Succeed

| https://www.eptac.com/webinars/tempered-leads-class-3-rework-toe-fillets-and-more/

. Definition of Class III Rework. Dissecting Toe Fillets on Gull Wing components. Understanding Gold Plating vs. Gold Flash. Have a question about training or IPC certification

  1 2 3 4 5 Next

enig flash gold searches for Companies, Equipment, Machines, Suppliers & Information

Sell Used SMT & Test Equipment

High Precision Fluid Dispensers
SMT feeders

High Throughput Reflow Oven
Software for SMT

World's Best Reflow Oven Customizable for Unique Applications