| https://www.eptac.com/faqs/soldertips/soldertip/soldertips-solderability-issues-with-nickle-plated-surfaces
: Solderability Issues with Nickle Plated Surfaces Question: We are working with components with leads of tin/lead over nickel. After the manufacturing processes, some of the pins are exhibiting what appears to be flaking plating, leaving behind unsolderable surfaces
| https://www.eptac.com/faqs/ask-helena-leo/ask/maximum-limits-of-solder-bath-contamination
: If we are using a solder pot to tin wires and create solder joints (splices), what Maximum Limits of Solder Bath Contaminant do we adhere to
Imagineering, Inc. | https://www.pcbnet.com/quote/board-quote/?cpn=0
* Materials FR4(130Tg) FR4(170Tg) Copper Weight 1 oz 2 oz 3 oz 4 oz Finish Plating HASL (Leaded) LF HASL Immersion Gold Immersion Silver White Tin OSP Minimum Trace/Space 0.005" 0.006" 0.007
| https://www.eptac.com/soldertips/dealing-with-the-problems-of-soldering-iron-tips-breaking-down/
quite higher than the melting temperature of the good old 63/37 or 60/40 tin/lead alloy solder. We were wrong. Increasing the solder iron temperature did not help, in fact, it created more problems and tip usage went through the roof
| https://www.eptac.com/faqs/ask-helena-leo/ask/what-is-the-correct-way-to-fill-solder-cups
. They will tin the wire, set the wire in, press the iron on the... Question: I noticed a lot of my techs, while soldering cups, are not putting the soldering iron on the back of the cup, filling with solder, then adding the tinned wire
ASCEN Technology | https://www.ascen.ltd/Products/Solder_paste_printer/513.html
(including the rugged Mark Point), to adapt to tin, copper, gold, spray tin, FPC, and other types of different colors of the PCB. 3. Scraper printing system Slide type scraper system to improve operational stability and extend service life 4
Imagineering, Inc. | https://www.pcbnet.com/quote/board-quote/?cpn=5
* Materials FR4(130Tg) FR4(170Tg) Copper Weight 1 oz 2 oz 3 oz 4 oz Finish Plating HASL (Leaded) LF HASL Immersion Gold Immersion Silver White Tin OSP Minimum Trace/Space 0.005" 0.006" 0.007
| https://www.eptac.com/ask/what-is-the-correct-way-to-fill-solder-cups/
. They will tin the wire, set the wire in, press the iron on the wire/solder cup and add solder. I’m not too familiar with soldering cups, but I am thinking that this will cause solder to wick up into the jacket
| https://www.eptac.com/faqs/soldertips?hsLang=en
. Read More Gold Removal Issues with Hollow Cup Connectors General Tip Question: We are having a hard time with the removal of gold from hollow cup connectors
| https://www.eptac.com/faqs/soldertips
. Read More Gold Removal Issues with Hollow Cup Connectors General Tip Question: We are having a hard time with the removal of gold from hollow cup connectors