40731 | https://www.smta.org/harsh/Harsh-Environments-Conference-Program-2020.pdf
Surface Mount Technology Association (SMTA)
| https://www.eptac.com/faqs/ask-helena-leo/ask/excess-flux-causing-intermittent-connection-issues
: We are having an issue with the cleanliness of flux. The excess no-clean flux is located in an Ethernet port connector. The units pass all tests with no issues, however
| https://www.smtfactory.com/PCBA-Cleaning-Machine-PCB-Defluxing-For-Best-Coating-and-Bonding-Effect-id43566387.html
cleaning is a full and important production step. But even with the so-called no-clean manufacturing, it may be that these components must be cleaned to avoid malfunctions
| https://www.eptac.com/soldertips/issues-of-burnt-flux-on-class-3-pcb-assemblies/
. I understand that if the laminate is burnt it is a defect condition, but I am not clear on burnt flux for a no-clean process. Any clarification would be appreciated. Answer
40731 | https://www.smta.org/harsh/Harsh-Environments-Program-2019.pdf?v=20052905555
Surface Mount Technology Association (SMTA)
40731 | https://www.smta.org/harsh/Harsh-Environments-Program-2019.pdf?v=20061608642
Surface Mount Technology Association (SMTA)
ASYMTEK Products | Nordson Electronics Solutions | https://www.nordson.com/en/divisions/select/technologies-or-options/microdrop-flux-dispenser
specific locations without overspray - Ideal for micro flux deposition of flux to small solder sites with unparalleled accuracy and minimal flux consumption - Provides true no-clean processing since flux is
| https://www.eptac.com/faqs/ask-helena-leo/page/8
. The excess no-clean flux is located in an Ethernet port connector. The units pass all tests with no issues, however; we have recently had a couple of field returns where it was
| https://www.eptac.com/soldertip/issues-of-burnt-flux-on-class-3-pcb-assemblies/
: Clean vs No-Clean Fluxes SolderTip #39: Class 2 vs Class 3 Assemblies SolderTip #40: Component Mounting and Acceptability Question
| https://www.eptac.com/soldertip/soldertips-solderability-issues-with-nickle-plated-surfaces/