Imagineering, Inc. | https://www.pcbnet.com/blog/understanding-the-pcb-fabrication-process-from-design-to-delivery/
. For example, electroless nickel immersion gold (ENIG) is a common surface finish due to its long shelf life and RoHS compliance . However, it’s more expensive than other options
. Does the IPC cover anything on shelf life of soldered components? Read Answer Training in Wire Bonding Question: Do you offer training in wire bonding
ASYMTEK Products | Nordson Electronics Solutions | https://www.nordson.com/en/divisions/efd/resource-center/solder-glossary-of-terms
with an appropriate solvent. Rosin/Resin (R) Natural or modified pine tree sap. Resins are processed Rosins. Rosin is the mildly acidic sap found in pine trees and was the first fluxing agent used in the Bronze Age. S Shelf Life Duration of time a
ORION Industries | http://orionindustries.com/pdfs/200mp.pdf
. Shelf Life of Tape in Roll Form 24 months from the manufacturing date when stored at 70°F (21°C) and 50% relative humidity. VI. Adhesion Retention after Immersion and Exposure (percent retention
ORION Industries | http://orionindustries.com/pdfs/300lse.pdf
: When properly applied, nameplates and decorative trim parts are not adversely affected by exposure. Water Resistance: Immersion in water has no appreciable effect on the bond strength
Heller Industries Inc. | https://hellerindustries.com/wp-content/uploads/2018/07/last-will-of-bga-void.pdf
. An opposing school of thought was that voids act as crack arrestors, which improve solder joint life. The root cause of voids in BGA solder joints is well understood by the electronics industry with a number of papers published on the topic [1, 2, 3]. R
Heller Industries Inc. | https://hellerindustries.com/wp-content/uploads/2022/04/last-will-of-bga-void-1.pdf
. An opposing school of thought was that voids act as crack arrestors, which improve solder joint life. The root cause of voids in BGA solder joints is well understood by the electronics industry with a number of papers published on the topic [1, 2, 3]. R
Surface Mount Technology Association (SMTA) | https://www.smta.org/knowledge/journal.cfm
, David Braun Abstract 22-2 EFFECTS OF STORAGE PROCEDURES AND BAKE OUT ON THE SOLDERABILITY OF IMMERSION SILVER-COATED PRINTED CIRCUIT BOARDS Paul Vianco, et al. Abstract 22-1 A CASE STUDY FOR TRANSITIONING CLASS A SERVER MOTHERBOARDS TO LEAD-FREE R
ASYMTEK Products | Nordson Electronics Solutions | https://www.nordson.com/en/divisions/efd/resources/solder-dictionary-of-terms
appropriate solvent. Rosin/Resin (R) Natural or modified pine tree sap. Resins are processed Rosins. Rosin is the mildly acidic sap found in pine trees and was the first fluxing agent used in the Bronze Age. S Shelf Life Duration of time a product remains
| https://pcbasupplies.com/leaded-solder-wire/
× 105 Flux residue stickiness (by chalk powder) No attachment Wire diameter (mm) 0.3, 0.4, 0.5, 0.6, 0.8, 1.0, 1.2, 1.6 Shelf life 3 years More Flux Cored Solder Wire Products JM-20 Sn63/Pb37